Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Tensile Modulus = 4.62 GPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Modulus 4.62 GPa
670 ksi
Type I, 5.1 mm/min; ASTM D638
PolyOne Edgetek® X TR2-30TA/000 NATURAL Copolyester
The Edgetek™ engineering thermoplastics compounds made with Eastman Tritan™ copolyester offer a wide range of performance and properties with the addition of reinforcing additives. By utilizing Ea..
Tensile Modulus 4.62 GPa
670 ksi
Type 1 - Rigids, 0.2 in/min; ASTM D638
PolyOne Edgetek® MLS-10GF/000 Polysulfone Alloy - 10% Glass Fiber Reinforced  (discontinued **)
Data provided by PolyOne.
Tensile Modulus 4.62 GPa
670 ksi
ASTM D638
Plastics Group Polifil® GFABS-10 10% Glass-Reinforced Acrylonitrile-Butadiene Styrene (ABS)
Polifil® GFABS series compounds combine the most desirable properties of both components - allowing for enhanced processability and toughness together with the stiffness of glass.Applications: Fire..
Tensile Modulus 4.62 GPa
670 ksi
ISO 527
Azdel Plus C321-B01 32% Chopped Fiber Mat / PP Resin Matrix
AZDEL® C321-B01 is a glass mat thermoplastic laminate based upon a random oriented chopped fiber mat contained within a polypropylene resin matrix. This composite material features high flow prope..
Copyright © lookpolymers.com All Rights Reserved