Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 4.70 GPa | 682 ksi | STN EN ISO 527-2 |
Plastcom PLASTAMID® 66 GF 15 T 15 TS PA66 reinforced with glass fibers and mineral filler, heat stabilized Black PA66 for injection molding, reinforced with 15% glass fiber and 15% mineral filler, for moldings used in the automotive, electrical, building, engineering and hobby industry - holders of elect.. |
|||
Tensile Modulus | 4.70 GPa | 682 ksi | |
Plastcom SLOVAMID 66 GB 30 LS PA66, 30% glass beads, light stability Packaging, transport, stockingThe product is packed in hermetically closed thick-walled 25 kg PE bags, on a 1.000 kg palette coated in a stretch foil, in big bags with a thick PE foil fixed on a 1.0.. |
|||
Tensile Modulus | 4.70 GPa @Thickness 4.00 mm, Temperature 23.0 °C |
682 ksi @Thickness 0.157 in, Temperature 73.4 °F |
Injection Molded; ISO 527-2 |
PolyOne Bergadur™ PB400 G10 H UF UV Polybutylene Terephthalate (PBT) Information provided by PolyOne |
|||
Tensile Modulus | 4.70 GPa | 682 ksi | STN EN ISO 527-2 |
Plastcom SLOVALEN PH 49 GF 20 Polypropylene Homopolymer, 20% Glass Fiber FeaturesModified homopolymer PP for injection moulding, chemically reinforced with 20% glass fiber, contains the modifier of mechanical properties. Increased strength in comparison with unfilled PP.. |
|||
Tensile Modulus | 4.70 GPa | 682 ksi | |
LATI Laticonther 52/11 CP3/600 F3 PP Homopolymer High thermal conductivity product based on Polypropylene homopolymer (PPh). Special filler. Potentially suitable for food/medical contact application.Availability: Africa & Middle East; Asia Pacific.. |
|||
Tensile Modulus | 4.70 GPa | 682 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics NORYL V02570 PPE+HIPS Noryl* V02570 is a 25% milled fiber reinforced, injection moldable grade. Designed for good dimensional stability and low warpage, this resin also uses non-chlorinated, non-brominated FR additives t.. |
|||
Tensile Modulus | 4.70 GPa | 682 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics NORYL V02570 PPE+HIPS (Europe-Africa-Middle East) Noryl* V02570 is a 25% milled fiber reinforced, injection moldable grade. Designed for good dimensional stability and low warpage, this resin also uses non-chlorinated, non-brominated FR additives t.. |
|||
Tensile Modulus | 4.70 GPa | 682 ksi | 5 mm/min; ASTM D638 |
SABIC Innovative Plastics LNP THERMOCOMP DX07350 PC (Asia Pacific) Lexan *DX07350 resin is a glass filled, Non-brominated & Non-chlorinated flame retardant polycarbonate. High stiffness and good flow. |
|||
Tensile Modulus | 4.70 GPa | 682 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP Thermocomp MF004S PP (Europe-Africa-Middle East) LNP* THERMOCOMP* MF004S is a compound based on Polypropylene resin, containing Glass Fiber. Added features include; Chemically Coupled.This data was supplied by SABIC-IP for the Europe-Africa-Middle.. |
|||
Tensile Modulus | 4.70 GPa | 682 ksi | ASTM D 638 |
Cossa Polimeri ESTAPROP H 0560 GFCTG Polypropylene, 30% Mixed Filler PP homopolymer 30% mixed fillerGood physical and mechanical characteristicsInformation provided by Cossa Polimeri S.r.l. |
|||
Tensile Modulus | 4.70 GPa | 682 ksi | ISO 527-1/-2 |
DSM Arnite® TM4 440 (PBT+PET)-MD20 20% Mineral Reinforced |
|||
Tensile Modulus | 4.70 GPa @Temperature 180 °C |
682 ksi @Temperature 356 °F |
ISO 527-1/-2 |
DSM Stanyl® 46HF4530 PA46-GF30 30% Glass Reinforced, Heat Stabilized, High Flow, for E&E applications |
|||
Tensile Modulus | 4.70 GPa | 682 ksi | 50mm/min; ISO 527-1 |
Denka TH-11 Transparent Resin Polymer (MBS resin) Polymethacrylate Butadiene Styrene "TX Polymer" (methyl methacrylate styrene), MS resins as an alternative to acrylic resins, with low density, low moisture absorption, and good moldability, "TH Polymer/TP Polymer," MBS resins with a.. |
|||
Tensile Modulus | 4.70 GPa | 682 ksi | 50mm/min; ISO 527-1 |
Denka TP-801 Transparent Resin Polymer (MBS resin) Polymethacrylate Butadiene Styrene "TX Polymer" (methyl methacrylate styrene), MS resins as an alternative to acrylic resins, with low density, low moisture absorption, and good moldability, "TH Polymer/TP Polymer," MBS resins with a.. |
|||
Tensile Modulus | 4.70 GPa | 682 ksi | ISO 527-1/-2 |
DuPont Performance Polymers Rynite® 415HP NC010 Polyethylene Terephthalate (PET)
(Unverified Data**) 15% Glass Reinforced Polyethylene Terephthalate with Excellent Impact Resistance Rynite 415HP NC010 is a 15% glass reinforced modified polyethylene terephthalate improved for easy fast processing ov.. |
|||
Tensile Modulus | 4.70 GPa | 682 ksi | 50%RH; ISO 527-1/-2 |
DuPont Performance Polymers Zytel® 80G25HS BK117 Nylon 66
(Unverified Data**) 25% Glass Reinforced Toughened Heat Stabilized Polyamide 66 Zytel 80G25HS BK117 is a 25% glass fiber reinforced toughened heat stabilized black polyamide 66 resin for injection molding.Information p.. |
|||
Tensile Modulus | 4.70 GPa | 682 ksi | 1 mm/min; ISO 527 |
Eurostar Starpylen MF004S PP, 20% Glass Fiber Filled, Injection Molded Starpylen MF004S is a 20% Glass Fiber Reinforced Polypropylene Injection Molding ResinInformation provided by Eurostar. |
|||
Tensile Modulus | 4.70 GPa | 682 ksi | ISO 527-1 |
Barlog Plastics KEBAFORM C 8027 POM Copolymer, 30% mineral reinforced POM-MD30Information provided by BARLOG plastics GmbH. |
|||
Tensile Modulus | 4.70 GPa | 682 ksi | |
BASF Procom® GC20H 250 Polypropylene Uses: car and truck fans and shrouds, car rear light housings, car radiator expansion tanks, car grills, domestic appliance components (e.g. washing machine tanks, impellers housings, etc.), textile.. |
|||
Tensile Modulus | 4.70 GPa | 682 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP THERMOTUF WF003I PBT (Europe-Africa-Middle East) LNP* Thermotuf* WF003I BLACK is a compound based on Polybutylene Terephalate resin containing Glass Fiber. Added features of this material include: High Impact. |