Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Modulus 2.832 GPa
410.8 ksi
ASTM D-638
Axiall 8266 Rigid PVC, Extrusion
Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013.
Tensile Modulus 2.832 GPa
410.8 ksi
ASTM D-638
Axiall 8266 Rigid PVC, Extrusion, Natural
Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013.
Tensile Modulus 2.832 GPa
410.8 ksi
ASTM D-638
Axiall 8266 Rigid PVC, Extrusion, White
Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013.