Material Notes:
Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013.
Physical Properties Metric English Comments
Specific Gravity 1.41 g/cc
1.41 g/cc
ASTM D-792
Mechanical Properties Metric English Comments
Hardness, Rockwell R 90
90
ASTM D-785
Hardness, Shore D 78
78
ASTM D-2240
Tensile Strength, Yield 39.41 MPa
5716 psi
ASTM D-638
Tensile Modulus 2.832 GPa
410.8 ksi
ASTM D-638
Flexural Strength 74.5 MPa
10800 psi
ASTM D-790
Flexural Modulus 2.614 GPa
379.2 ksi
ASTM D-790
Izod Impact, Notched 1.43 J/cm

@Thickness 6.35 mm
2.68 ft-lb/in

@Thickness 0.250 in
ASTM D-256
1.89 J/cm

@Thickness 3.17 mm
3.54 ft-lb/in

@Thickness 0.125 in
ASTM D-256
Tensile Impact Strength 115 kJ/m²
55.0 ft-lb/in²
ASTM D-1822
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 60.0 °C
140 °F
unannealed; ASTM D-648
67.8 °C
154 °F
annealed; ASTM D-648
Processing Properties Metric English Comments
Melt Temperature 188 °C
370 °F
Descriptive Properties Value Comments
Cell Classification 13253
ASTM D-1784