Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 3.09 GPa | 448 ksi | Type I, 5.1 mm/min; ASTM D638 |
PolyOne Geon™ Vinyl Dry Blend E7456 Polyvinyl Chloride, Rigid (PVC, Rigid) Information provided by PolyOne |
|||
Tensile Modulus | 3.09 GPa @Temperature 80.0 °C |
448 ksi @Temperature 176 °F |
ISO Data |
BASF Ultramid® 8267G HS BK-106 15/25% Glass/Mineral Filled PA6 (Dry) Ultramid 8267G HS BK-106 is a heat stabilized, weather resistant, 40% mineral and glass fiber reinforced PA6 injection molding compound with improved UV resistance and sink mark resistance. The com.. |
|||
Tensile Modulus | 3.09 GPa | 448 ksi | ASTM D-638 |
Axiall 7407 Rigid PVC, Extrusion Georgia Gulf 7407 is a rigid PVC compound designed for outdoor applications.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013. |