Polymer Property : Tensile Modulus = 451 ksi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Modulus 3.11 GPa
451 ksi
1 mm/min; ISO 527
SABIC Innovative Plastics EXTEM VH1003 PEI Copolymer
Transparent, Thermoplastic Polyimide (TPI) resin with a glass transition temperature (Tg) of 247C. This product has thinwall FR capability and has a UL94 V0 listing. This material is RoHS compliant..
Tensile Modulus 3.11 GPa
451 ksi
1 mm/min; ISO 527
SABIC Innovative Plastics EXTEM VH1003 PEI Copolymer (Asia Pacific)
Transparent, Thermoplastic Polyimide (TPI) resin. Glass transition Temp. (Tg) of 247°C. This resin has thinwall FR capability and has a UL94 V0 listing. Resin is RoHS compliant and halogen free acc..
Tensile Modulus 3.11 GPa
451 ksi
1 mm/min; ISO 527
SABIC Innovative Plastics EXTEM VH1003 PEI Copolymer (Europe-Africa-Middle East)
Transparent, Thermoplastic Polyimide (TPI) resin. Glass transition Temp. (Tg) of 247°C. This resin has thinwall FR capability and has a UL94 V0 listing. Resin is RoHS compliant and halogen free acc..
Tensile Modulus 3.11 GPa
451 ksi
1 mm/min; ISO 527
SABIC Innovative Plastics EXTEM VH1003F PEI Copolymer
Transparent, Thermoplastic Polyimide (TPI) resin with a glass transition temperature (Tg) of 247C. This product has thinwall FR capability and has a UL94 V0 listing. This material is RoHS compliant..
Tensile Modulus 3.11 GPa
451 ksi
1 mm/min; ISO 527
SABIC Innovative Plastics EXTEM VH1003F PEI Copolymer (Europe-Africa-Middle East)
Transparent, Thermoplastic Polyimide (TPI) resin. Glass transition Temp. (Tg) of 247°C. Global Food Contact Approval. Resin is subject to Commerce Control Laws U.S. 15CFR Chapter VII, Part 774 and ..
Tensile Modulus 3.11 GPa
451 ksi
1 mm/min; ISO 527
SABIC Innovative Plastics EXTEM VH1003P PEI Copolymer
Transparent, Thermoplastic Polyimide (TPI) resin with a glass transition temperature (Tg) of 247C. Powder version of VH1003. This resin is a Dual-use item and is subject to export control restrictio..
Tensile Modulus 3.11 GPa
451 ksi
1 mm/min; ISO 527
SABIC Innovative Plastics EXTEM VH1003P PEI Copolymer (Asia Pacific)
Transparent, Thermoplastic Polyimide (TPI) resin with a glass transition temperature (Tg) of 247C. Powder version of VH1003. This resin is a Dual-use item and is subject to export control restrictio..
Tensile Modulus 3.11 GPa
451 ksi
1 mm/min; ISO 527
SABIC Innovative Plastics EXTEM VH1003P PEI Copolymer (Europe-Africa-Middle East)
Transparent, Thermoplastic Polyimide (TPI) resin with a glass transition temperature (Tg) of 247C. Powder version of VH1003. This resin is a Dual-use item and is subject to export control restrictio..
Tensile Modulus 3.11 GPa
451 ksi
1 mm/min; ISO 527
SABIC Innovative Plastics LNP FARADEX WX94736 PBT
LNP* Faradex* WX94736 is a compound based on Polybutylene Terephalate resin containing Stainless Steel.
Tensile Modulus 3.11 GPa
451 ksi
1 mm/min; ISO 527
SABIC Innovative Plastics EXTEM VH1003F PEI Copolymer (Asia Pacific)
Transparent, Thermoplastic Polyimide (TPI) resin. Glass transition Temp. (Tg) of 247°C. Global Food Contact Approval. Resin is subject to Commerce Control Laws U.S. 15CFR Chapter VII, Part 774 and ..
Tensile Modulus 3.11 GPa

@Thickness 3.20 mm
451 ksi

@Thickness 0.126 in
1 mm/min; ASTM D638
LG Chemical 80HF SAN, High Transparency, Heat Resistance, Chemical Resistance
Feature: Injection Molding, SAN, High Transparency, Heat Resistance, Chemical ResistanceApplication: Refrigerator Sleeves, MiscellaneousCAS No. 9003-54-7Information provided by LG Chemical
Tensile Modulus 3.11 GPa

@Thickness 3.20 mm
451 ksi

@Thickness 0.126 in
1 mm/min; ASTM D638
LG Chemical 80HFICELLHK SAN, High Transparency, Heat Resistance, Chemical Resistance
Feature: Injection Molding, SAN, High Transparency, Heat Resistance, Chemical ResistanceApplication: Refrigerator Sleeves, MiscellaneousCAS No. 9003-54-7Information provided by LG Chemical
Tensile Modulus 3.11 GPa
451 ksi
1 mm/min; ISO 527
SABIC Innovative Plastics ULTEM AUT230 PEI (Europe-Africa-Middle East)
Transparent polyetherimide (Tg 247 degC). Very low outgassing and plateout, for automotive lighting applications where highly metallized, reflective surfaces are required. Haze onset temperature of..
Tensile Modulus 3.11 GPa
451 ksi
1 mm/min; ISO 527
SABIC Innovative Plastics ULTEM XH6050 PEI Copolymer
Transparent, enhanced flow Polyetherimidesulfone copolymer (Tg 247C). ECO Conforming, UL94 V0 listing. Resin is subject to U.S. Commerce Control Laws (15CFR Chapter VII, Part 774).
Tensile Modulus 3.11 GPa
451 ksi
1 mm/min; ISO 527
SABIC Innovative Plastics ULTEM XH6050 PEI Copolymer (Asia Pacific)
Transparent, enhanced flow Polyetherimidesulfone copolymer (Tg 247C). ECO Conforming, UL94 V0 listing. Resin is subject to U.S. Commerce Control Laws (15CFR Chapter VII, Part 774).
Tensile Modulus 3.11 GPa
451 ksi
1 mm/min; ISO 527
SABIC Innovative Plastics Ultem XH6050 PEI Copolymer (Europe-Africa-Middle East)
Transparent, enhanced flow Polyetherimidesulfone copolymer (Tg 247C). ECO Conforming, UL94 V0 listing. Resin is subject to U.S. Commerce Control Laws (15CFR Chapter VII, Part 774).This data was su..
Tensile Modulus 3.11 GPa
451 ksi
1 mm/min; ISO 527
SABIC Innovative Plastics ULTEM XH6050F PEI Copolymer
Transparent, enhanced flow Polyetherimidesulfone copolymer (Tg 247C). ECO Conforming. US FDA Compliant. Resin is subject to U.S. Commerce Control Laws (15CFR Chapter VII, Part 774).
Tensile Modulus 3.11 GPa
451 ksi
1 mm/min; ISO 527
SABIC Innovative Plastics ULTEM XH6050F PEI Copolymer (Asia Pacific)
Transparent, enhanced flow Polyetherimidesulfone copolymer (Tg 247C). ECO Conforming. US FDA Compliant. Resin is subject to U.S. Commerce Control Laws (15CFR Chapter VII, Part 774).
Tensile Modulus 3.11 GPa
451 ksi
1 mm/min; ISO 527
SABIC Innovative Plastics Ultem XH6050F PEI Copolymer (Europe-Africa-Middle East)
Transparent, enhanced flow Polyetherimidesulfone copolymer (Tg 247C). ECO Conforming. US FDA Compliant. Resin is subject to U.S. Commerce Control Laws (15CFR Chapter VII, Part 774).This data was ..
Tensile Modulus 3.11 GPa
451 ksi
1 mm/min; ISO 527
SABIC Innovative Plastics ULTEM AUT230 PEI
Transparent polyetherimide (Tg 247 degC). Very low outgassing and plateout, for automotive lighting applications where highly metallized, reflective surfaces are required. Haze onset temperature of..
Tensile Modulus 3.11 GPa
451 ksi
1 mm/min; ISO 527
SABIC Innovative Plastics ULTEM AUT230 PEI (Asia Pacific)
Transparent polyetherimide (Tg 247 degC). Very low outgassing and plateout, for automotive lighting applications where highly metallized, reflective surfaces are required. Haze onset temperature of..
Tensile Modulus 3.11 GPa
451 ksi
1 mm/min; ISO 527
SABIC Innovative Plastics NORYL EXNL0143 PPE+PS
Noryl PX1736 Resin is a blend of PPE and PS, that provides high strength, increased heat resistance, and translucency. The material has melt strenght suitable for Extrusion and Blow Molding applica..
Tensile Modulus 3.11 GPa
451 ksi
1 mm/min; ISO 527
SABIC Innovative Plastics NORYL PX1736 PPE+PS
Noryl PX1736 Resin is a blend of PPE and PS, that provides high strength, increased heat resistance, and translucency. The material has melt strenght suitable for Extrusion and Blow Molding applica..
Tensile Modulus 3.11 GPa
451 ksi
ASTM D638
Aclo Accutech Polypropylene Homopolymer HP0334G10M20CL Glass/Mineral Reinforced Coupled