SABIC Innovative Plastics LNP FARADEX WX94736 PBT

Category Polymer , Thermoplastic , Polyester, TP , Polybutylene Terephthalate (PBT)
Manufacturer SABIC Innovative Plastics (GE Plastics)
Trade Name LNP FARADEX
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF SABIC Innovative Plastics LNP FARADEX WX94736 PBT.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
LNP* Faradex* WX94736 is a compound based on Polybutylene Terephalate resin containing Stainless Steel.
Physical Properties Metric English Comments
Density 1.50 g/cc
0.0542 lb/in³
ISO 1183
1.51 g/cc
0.0546 lb/in³
ASTM D792
Moisture Absorption 0.100 %
0.100 %
50% RH, 24 hrs; ASTM D570
Linear Mold Shrinkage, Flow 0.0089 cm/cm

@Time 86400 sec
0.0089 in/in

@Time 24.0 hour
ISO 294
0.0080 - 0.010 cm/cm

@Time 86400 sec
0.0080 - 0.010 in/in

@Time 24.0 hour
ASTM D955
Linear Mold Shrinkage, Transverse 0.010 - 0.012 cm/cm

@Time 86400 sec
0.010 - 0.012 in/in

@Time 24.0 hour
ASTM D955
0.011 cm/cm

@Time 86400 sec
0.011 in/in

@Time 24.0 hour
ISO 294
Mechanical Properties Metric English Comments
Tensile Strength at Break 53.0 MPa
7690 psi
ASTM D638
53.0 MPa
7690 psi
ISO 527
Tensile Strength, Yield 53.0 MPa
7690 psi
ASTM D638
53.0 MPa
7690 psi
ISO 527
Elongation at Break 2.8 %
2.8 %
ASTM D638
2.9 %
2.9 %
ISO 527
Elongation at Yield 2.7 %
2.7 %
ASTM D638
2.8 %
2.8 %
ISO 527
Tensile Modulus 3.11 GPa
451 ksi
1 mm/min; ISO 527
3.44 GPa
499 ksi
50 mm/min; ASTM D638
Flexural Strength 55.0 MPa
7980 psi
ASTM D790
83.0 MPa
12000 psi
ISO 178
Flexural Modulus 2.75 GPa
399 ksi
ASTM D790
3.10 GPa
450 ksi
ISO 178
Izod Impact, Notched 0.580 J/cm
1.09 ft-lb/in
ASTM D256
Izod Impact, Unnotched 6.14 J/cm
11.5 ft-lb/in
ASTM D4812
Izod Impact, Notched (ISO) 6.00 kJ/m²
2.86 ft-lb/in²
80*10*4; ISO 180/1A
Izod Impact, Unnotched (ISO) 22.0 kJ/m²
10.5 ft-lb/in²
80*10*4; ISO 180/1U
Dart Drop, Total Energy 6.00 J
4.43 ft-lb
Instrumented Impact Energy @ peak; ASTM D3763
Impact Test 1.00 J
0.738 ft-lb
Multiaxial Impact; ISO 6603
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 82.8 µm/m-°C

@Temperature -40.0 - 40.0 °C
46.0 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
83.0 µm/m-°C

@Temperature -40.0 - 40.0 °C
46.1 µin/in-°F

@Temperature -40.0 - 104 °F
ISO 11359-2
CTE, linear, Transverse to Flow 68.4 µm/m-°C

@Temperature -40.0 - 40.0 °C
38.0 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
69.0 µm/m-°C

@Temperature -40.0 - 40.0 °C
38.3 µin/in-°F

@Temperature -40.0 - 104 °F
ISO 11359-2
Deflection Temperature at 0.46 MPa (66 psi) 147 °C
297 °F
Flatw 80*10*4 sp=64mm; ISO 75/Bf
143 °C

@Thickness 3.20 mm
289 °F

@Thickness 0.126 in
unannealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 123 °C
253 °F
Flatw 80*10*4 sp=64mm; ISO 75/Af
99.0 °C

@Thickness 3.20 mm
210 °F

@Thickness 0.126 in
unannealed; ASTM D648
Electrical Properties Metric English Comments
Volume Resistivity 3.0 - 7.0 ohm-cm
3.0 - 7.0 ohm-cm
ASTM D257
Surface Resistance 2.0 - 6.0 ohm
2.0 - 6.0 ohm
ASTM D257