Mechanical Properties Metric English Comments
Tensile Modulus 3.16 GPa
458 ksi
1 mm/min; ISO 527
SABIC Innovative Plastics EXTEM XH1005 TPI Resin
Thermoplastic Polyimide Extem* XH1005 Resin.
Tensile Modulus 3.16 GPa
458 ksi
1 mm/min; ISO 527
SABIC Innovative Plastics EXTEM XH1005 TPI Resin (Asia Pacific)
Thermoplastic Polyimide Extem* XH1005 Resin.
Tensile Modulus 3.16 GPa
458 ksi
1 mm/min; ISO 527
SABIC Innovative Plastics EXTEM XH1005 TPI Resin (Europe-Africa-Middle East)
Thermoplastic Polyimide Extem* XH1005 Resin.
Tensile Modulus 3.16 GPa
458 ksi
1 mm/min; ISO 527
SABIC Innovative Plastics EXTEM XH1005F TPI Resin (Europe-Africa-Middle East)
High Heat Amorphous TPI Blend, Tg 267C, High Continuous Use Temperature (CUT). EFSA Food Contact Approved. Material is UL listed. This material is RoHS compliant and also halogen free according VDE/..
Tensile Modulus 3.16 GPa
458 ksi
50 mm/min; ASTM D638
SABIC Innovative Plastics LNP LUBRICOMP IAL12 PA6.12
LNP* LUBRICOMP* IAL12 is a compound based on Nylon 6/12 resin containing 5% PTFE, 10% Aramid Fiber. Added features of this material include: Internally Lubricated.
Tensile Modulus 3.16 GPa
458 ksi
1 mm/min; ISO 527
SABIC Innovative Plastics LNP LUBRICOMP LX00430 PEEK
LNP* LUBRICOMP* LX00430 is a compound based on Pelyetheretherketone containing Proprietary Fillers. Added feature of this grade is: Wear Resistant.
Tensile Modulus 3.16 GPa
458 ksi
1 mm/min; ISO 527
SABIC Innovative Plastics LNP Lubricomp RL0049 PA 66
LNP* Lubricomp* RL0049 is a compound based on Nylon 66 resin containing PTFE, Flame Retardant. Added features of this material include: Internally Lubricated, Flame Retardant.This data was supplied..
Tensile Modulus 3.16 GPa
458 ksi
1 mm/min; ISO 527
SABIC Innovative Plastics LNP LUBRICOMP RL0049S PA 66
LNP LUBRICOMP* RL0049S is a compound based on Nylon 66 resin containing 20% PTFE. Added features of this material include: Flame Retardant, Heat Stabilized, Wear Resistant.
Tensile Modulus 3.16 GPa
458 ksi
1 mm/min; ISO 527
SABIC Innovative Plastics LNP THERMOCOMP 9X07430 PBT+PC
LNP* THERMOCOMP* 9X07430 is a compoud based on a PBT+PC Blend containing Glass Fiber, Talc. Added features of this material include: Opaque, Weatherable.