Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 3.28 GPa | 475 ksi | ASTM D638 |
Quantum Nylon 6/6 MoS2 Filled Information provided by Quantum Advanced Engineering Plastics |
|||
Tensile Modulus | 3.28 GPa | 475 ksi | ASTM D882 |
Westlake Plastics Tempalux® Film Made from ULTEM® Polyetherimide Resin High heat deflection and continuous use temperature. Inherent flame resistance. Extremely low NBS smoke evolution & superior limiting oxygen index.Ultem® is a trade name of GE Plastics. Informat.. |
|||
Tensile Modulus | 3.28 GPa | 475 ksi | ASTM D-638 |
Axiall 2512 Rigid PVC, Extrusion Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013. |