Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Tensile Modulus = 484 ksi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Modulus 3.34 GPa
484 ksi
1 mm/min; ISO 527
SABIC Innovative Plastics Cycoloy® C7410 PC+ABS (Asia Pacific)
Cycoloy* C7410 resin is a talc-filled PC+ABS, nonhalogenated FR for thinwall molding applications.
Tensile Modulus 3.34 GPa
484 ksi
5 mm/min; ASTM D638
SABIC Innovative Plastics ULTEM LTX300B PEI
Standard flow Polyetherimide blend with low toxicity, smoke, and flame evolution. ECO Compliant, UL94 V0 listing.
Tensile Modulus 3.34 GPa
484 ksi
5 mm/min; ASTM D638
SABIC Innovative Plastics ULTEM LTX300B PEI (Asia Pacific)
Standard flow Polyetherimide blend with low toxicity, smoke, and flame evolution. ECO Compliant, UL94 V0 listing.
Tensile Modulus 3.34 GPa
484 ksi
50 mm/min; ASTM D638
SABIC Innovative Plastics LNP STAT-KON FX98501 PE
LNP* STAT-KON* FX98501 is a compound based on Polyethylene resin containing Proprietary Fillers. Added feature of this material is: Electrically Conductive.
Tensile Modulus 3.34 GPa
484 ksi
1 mm/min; ISO 527
SABIC Innovative Plastics LNP Thermocomp C7410 PC+ABS (Asia Pacific)
LNP* Thermocomp* C7410 compound is a talc-filled PC+ABS, nonhalogenated FR for thinwall molding applications.This data was supplied by SABIC-IP for the Asia Pacific region.
Tensile Modulus 3.34 GPa
484 ksi
1 mm/min; ISO 527
SABIC Innovative Plastics LNP THERMOCOMP C7410 PC+ABS (Asia Pacific)
LNP* Thermocomp* C7410 compound is a talc-filled PC+ABS, nonhalogenated FR for thinwall molding applications.
Tensile Modulus 3.33 GPa
484 ksi
50 mm/min; ASTM D638
Samsung Cheil Industries Infino® NH-1150HH PC/ABS, Unreinforced FR
Information provided by Samsung Cheil Industries.
Tensile Modulus 3.33 GPa
484 ksi
50 mm/min; ASTM D638
Samsung Cheil Industries Infino® NH-1150HH PC/ABS, Unreinforced FR
Information provided by Samsung Cheil Industries.
Tensile Modulus 3.34 GPa
484 ksi
DIN EN ISO 527
Wolf Kunststoff ZEDEX® ZX-530CD3 031 Polymer Alloy, Fiber Reinforced and PTFE Modified
Main Characteristics: Dimensionally stable and rigid; Stress resistant; Extremely low wear to 100 ° CApplications: Chemical Engineering; Laboratory Technology; Automitve Technology; Machine ToolsIn..
Tensile Modulus 3.34 GPa
484 ksi
ASTM D-638
Axiall 7765 Rigid PVC, Extrusion
Georgia Gulf 7765 is a general-purpose indoor rigid PVC profile extrusion compound designed for applications requiring the following properties. 7765 carries an NSF standard 51 listing (for food zo..
Copyright © lookpolymers.com All Rights Reserved