Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

SABIC Innovative Plastics ULTEM LTX300B PEI (Asia Pacific)

Category Polymer , Thermoplastic , Polyetherimide (PEI)
Manufacturer SABIC Innovative Plastics (GE Plastics)
Trade Name ULTEM
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF SABIC Innovative Plastics ULTEM LTX300B PEI (Asia Pacific).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Standard flow Polyetherimide blend with low toxicity, smoke, and flame evolution. ECO Compliant, UL94 V0 listing.
Physical Properties Metric English Comments
Specific Gravity 1.27 g/cc
1.27 g/cc
ASTM D792
Halogen Content 0.00 %
0.00 %
SABIC Method
Linear Mold Shrinkage, Flow 0.0030 - 0.0050 cm/cm

@Thickness 3.20 mm
0.0030 - 0.0050 in/in

@Thickness 0.126 in
SABIC Method
Linear Mold Shrinkage, Transverse 0.0050 - 0.0070 cm/cm

@Thickness 3.20 mm
0.0050 - 0.0070 in/in

@Thickness 0.126 in
SABIC Method
Melt Flow 1.6 g/10 min

@Load 6.60 kg,
Temperature 295 °C
1.6 g/10 min

@Load 14.6 lb,
Temperature 563 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 96.0 MPa
13900 psi
Type I, 5 mm/min; ASTM D638
Elongation at Break 88 %
88 %
Type I, 5 mm/min; ASTM D638
Tensile Modulus 3.34 GPa
484 ksi
5 mm/min; ASTM D638
Flexural Strength 141 MPa
20500 psi
2.6 mm/min, 100 mm span; ASTM D790
Flexural Yield Strength 144 MPa
20900 psi
2.6 mm/min, 100 mm span; ASTM D790
Flexural Modulus 3.20 GPa
464 ksi
2.6 mm/min, 100 mm span; ASTM D790
Izod Impact, Notched 0.800 J/cm
1.50 ft-lb/in
ASTM D256
21.36 J/cm

@Thickness 3.20 mm
40.02 ft-lb/in

@Thickness 0.126 in
ASTM D256
Gardner Impact 35.0 J
25.8 ft-lb
ASTM D3029
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 190 °C

@Thickness 6.40 mm
374 °F

@Thickness 0.252 in
unannealed; ASTM D648
UL RTI, Electrical 140 °C
284 °F
UL 746B
UL RTI, Mechanical with Impact 115 °C
239 °F
UL 746B
UL RTI, Mechanical without Impact 140 °C
284 °F
UL 746B
Flammability, UL94 V-0

@Thickness 0.760 mm
V-0

@Thickness 0.0299 in
UL 94
Electrical Properties Metric English Comments
Arc Resistance 60 - 120 sec
60 - 120 sec
Tungsten; ASTM D495
Comparative Tracking Index 100 - 175 V
100 - 175 V
UL 746A
Hot Wire Ignition, HWI >= 120 sec
>= 120 sec
UL 746A
High Amp Arc Ignition, HAI >= 120 arcs
>= 120 arcs
UL 746A
High Voltage Arc-Tracking Rate, HVTR 80.0 - 150 mm/min
3.15 - 5.91 in/min
UL 746A
Users viewing this material also viewed the following: