Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 5.85 GPa | 848 ksi | 5 mm/min; ASTM D638 |
SABIC Innovative Plastics Cycoloy® CM6220 PC (Asia Pacific) CYCOLOY CM6220 resin is a mineral filled grade featuring of high modulus (6GPa), good flow and ductility, low warpage. It is of non-Br & non-Cl flame retardant systems intended to meet thin wall fla.. |
|||
Tensile Modulus | 5.85 GPa | 848 ksi | |
Radici Radilon® A CP400 (dry) Nylon 66 Radilon® A is a range of polyamide 66 (PA66) products obtained through the polymerization of hexamethylendiamine and adipic acid, and used for injection, extrusion and blow-molding.Information prov.. |
|||
Tensile Modulus | 5.85 GPa | 848 ksi | 5 mm/min; ASTM D638 |
SABIC Innovative Plastics Lexan® BM5225X PC (Asia Pacific) BM5225X resin is a mineral filled grade featuring of high modulus, good flow and ductility, low warpage. It is of non-Br & non-Cl flame retardant systems intended to meet thin wall flame resistance .. |
|||
Tensile Modulus | 5.85 GPa | 848 ksi | ISO 527-1/-2 |
Quadrant EPP Semitron® ESd 410C PEI, static dissipative, extruded (ISO Data) Having an excellent mechanical performance up to 210 °C, Semitron ESd 410C provides ESd-solutions at higher temperatures. Additionally, Semitron ESd 410C exhibits excellent dimensional stability (l.. |