Mechanical Properties Metric English Comments
Tensile Modulus 0.350 GPa
50.8 ksi
STN EN ISO 527-2
Plastcom PLASTALEN® TPU N 85 LTS TPU
Modified TPU. Use in all industry sectors. Delivered in the black.Information Provided by Plastcom spol. s r.o.
Tensile Modulus 0.350 GPa
50.8 ksi
ISO 527-1/-2
DSM Arnitel® UM622 General Purpose Grade Copolyester Elastomer (North America)  (discontinued **)
Product description: Arnitel® combines the advantages of engineering thermoplastics, being easy to process with excellent mechanical properties, at the same time with the flexibility of rubbers.Arn..
Tensile Modulus 0.350 GPa
50.8 ksi
ISO 527-1/-2
DSM Arnitel® UM622 Polyether Ester Elastomer (European Grade)  (discontinued **)
Product description: Arnitel® combines the advantages of engineering thermoplastics, being easy to process with excellent mechanical properties, at the same time with the flexibility of rubbers.Arn..
Tensile Modulus 0.350 GPa
50.8 ksi
LyondellBasell Lupolen® 3010 K LDPE, Injection Molding Grade
Injection moldingsData was collected by ISO methods and originally provided by BASF. The Lupolen® product line is now produced by Basell.
Tensile Modulus 0.350 - 0.700 GPa
50.8 - 102 ksi
DIN 53457
Isoflon FEP Fluorinated Ethylene Propylene
Fluoropolymer material specifications.Information provided by Isoflon.
Tensile Modulus 0.350 GPa
50.8 ksi
cond.; ISO 527-1, -2; 1 mm/min
Lanxess Durethan® BC 600 HTS DUSXBL 900116 Nylon 6, Impact Modified
PA 6, non-reinforced, extrusion, blow molding, impact modified, heat-aging stabilizedInformation provided by LANXESS.
Tensile Modulus 0.350 GPa

@Temperature 100 °C
50.8 ksi

@Temperature 212 °F
DIN 53457
Zell-Metall Engineering Plastics Zellamid 1100 OIL at 50% RH
Zellamid® 1100 OIL: A new type of cast nylon produced by addition of a special oil to the polymer structure. By laboratory test it was proven that this second generation oil filled product reduces ..
Tensile Modulus 0.350 - 0.450 GPa
50.8 - 65.3 ksi
MD/TD; ISO 527-3
Borealis BorPURE™ RD208CF Polypropylene Random Copolymer
BorPure™ RD208CF is a random copolymer. This grade is suitable for the manufacturing of unoriented films on chill roll processes. This grade is suitable for the manufacturing of unoriented films o..
Tensile Modulus 0.350 GPa
50.8 ksi
conditioned; ISO 527-1/-2
EMS-Grivory Grivory® BRZ 347 W PA6
Product description: Grilon BRZ 347 W is a heat stabilized, high viscosity, impact modified and plasticized PA6 extrusion grade. Grilon BRZ 347 W has the following important properties: High flexibi..
Tensile Modulus 0.350 GPa
50.8 ksi
conditioned; ISO 527-1/-2
EMS-Grivory Grivory® XE 3841 nat PA12
Product description: Grilamid XE 3841 is a flexible, heat stabilized and plasticizer-free Polyamide 12, which offers a very good processability for extrusion. Grilamid XE 3841 is qualified in Europe..
Tensile Modulus 0.350 GPa
50.8 ksi
conditioned; ISO 527-1/-2
EMS-Grivory Grivory® CA 6 E PA*
Product description: Grilon CA 6 E is a non-extracted copolyamide with a low melting point. Grilon CA 6 E characterizes itself through the following properties Very high flexibility and toughnessVer..
Tensile Modulus 0.350 GPa
50.8 ksi
conditioned; ISO 527-1/-2
EMS-Grivory Grivory® L 25 W 40 ESD PA12
Product Description: Grilamid L 25 W 40 ESD is a high viscosity, anti-static highly flexible extrusion grade of Polyamide 12 (PA12). Grilamid L 25 W 40 ESD is plasticized and heat stabilized The inh..
Tensile Modulus 0.350 GPa
50.8 ksi
dry; ISO 527-1/-2
EMS-Grivory Grivory® L 25 W 40 ESD PA12
Product Description: Grilamid L 25 W 40 ESD is a high viscosity, anti-static highly flexible extrusion grade of Polyamide 12 (PA12). Grilamid L 25 W 40 ESD is plasticized and heat stabilized The inh..
Tensile Modulus 0.350 GPa

@Temperature 120 °C
50.8 ksi

@Temperature 248 °F
50%RH; ISO 11403-1 -2
DuPont Performance Polymers Zytel® 151L NC010 Nylon 612  (Unverified Data**)
Unreinforced Polyamide 612Information provided by DuPont Performance Polymers
Tensile Modulus 0.350 GPa
50.8 ksi
Arkema Group KYNAR FLEX® 2800-00 Polyvinylidene Fluoride Copolymer - Extrusion
Characteristics: Natural resin - translucent, off-white hemispheres. Flexible. High stability in harsh thermal, chemical and ultraviolet environments. High toughness and mechanical strength, low..
Tensile Modulus 0.350 GPa
50.8 ksi
ISO 527-2
CENTROPLAST CENTROMID 12 LE soft Polyamide 12 LE soft
This extruded material is suitable for conveying foodstuffs and pharmaceutical products. It is used in flexible tubes for worm gears and spiral conveyors.Information provided by CENTROPLAST Enginee..