Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

EMS-Grivory Grivory® L 25 W 40 ESD PA12

Category Polymer , Thermoplastic , Nylon , Nylon 12
Manufacturer EMS-Grivory (EMS-CHEMIE)
Trade Name Grivory®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF EMS-Grivory Grivory® L 25 W 40 ESD PA12.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Product Description: Grilamid L 25 W 40 ESD is a high viscosity, anti-static highly flexible extrusion grade of Polyamide 12 (PA12). Grilamid L 25 W 40 ESD is plasticized and heat stabilized The inherent color of this material is black. The main features of Grilamid L 25 W 40 ESD are: Anti-staticHighly flexibleGood heat stabilityGood dimensional stabilityEasy processingLow density, low weight Application examples: Grilamid L 25 W 40 ESD is suitable for the production of highly flexible tubes and profiles having anti-static properties for use in automotive and industrial applications.Information provided by EMS Grivory
Physical Properties Metric English Comments
Density 1.04 g/cc
0.0376 lb/in³
ISO 1183
Water Absorption 1.1 %
1.1 %
ISO 62
Moisture Absorption 0.600 %
0.600 %
ISO 62
Linear Mold Shrinkage, Flow 0.011 cm/cm
0.011 in/in
ISO 294-4, 2577
Linear Mold Shrinkage, Transverse 0.014 cm/cm
0.014 in/in
ISO 294-4, 2577
Mechanical Properties Metric English Comments
Hardness, Shore D 63
63
conditioned, 15s; ISO 868
Tensile Strength at Break 35.0 MPa
5080 psi
dry; ISO 527-1/-2
35.0 MPa
5080 psi
conditioned; ISO 527-1/-2
Tensile Strength, Yield 25.0 MPa
3630 psi
dry; ISO 527-1/-2
25.0 MPa
3630 psi
dry; ISO 527-1/-2
Elongation at Break >= 50 %
>= 50 %
conditioned; ISO 527-1/-2
<= 50 %
<= 50 %
dry; ISO 527-1/-2
Elongation at Yield 20 %
20 %
conditioned; ISO 527-1/-2
20 %
20 %
dry; ISO 527-1/-2
Tensile Modulus 0.350 GPa
50.8 ksi
conditioned; ISO 527-1/-2
0.350 GPa
50.8 ksi
dry; ISO 527-1/-2
Charpy Impact Unnotched NB
NB
dry; ISO 179/1eU
NB
NB
conditioned; ISO 179/1eU
NB

@Temperature 30.0 °C
NB

@Temperature 86.0 °F
dry; ISO 179/1eU
NB

@Temperature 30.0 °C
NB

@Temperature 86.0 °F
conditioned; ISO 179/1eU
Charpy Impact, Notched NB
NB
dry; ISO 179/1eA
NB
NB
conditioned; ISO 179/1eA
0.700 J/cm²

@Temperature 30.0 °C
3.33 ft-lb/in²

@Temperature 86.0 °F
dry; ISO 179/1eU
0.900 J/cm²

@Temperature 30.0 °C
4.28 ft-lb/in²

@Temperature 86.0 °F
conditioned; ISO 179/1eU
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 140 µm/m-°C
77.8 µin/in-°F
ISO 11359-1/-2
CTE, linear, Transverse to Flow 180 µm/m-°C
100 µin/in-°F
ISO 11359-1/-2
Melting Point 173 °C
343 °F
10°C/min; ISO 11357-1/-3
Maximum Service Temperature, Air 90.0 - 110 °C
194 - 230 °F
long term; EMS
150 °C
302 °F
short term; EMS
Deflection Temperature at 0.46 MPa (66 psi) 95.0 °C
203 °F
ISO 75-1/-2
Deflection Temperature at 1.8 MPa (264 psi) 45.0 °C
113 °F
ISO 75-1/-2
Flammability, UL94 HB
HB
IEC 60695-11-10
Electrical Properties Metric English Comments
Volume Resistivity 1e+05
1e+05
conditioned; IEC 60093
Surface Resistance 1.00e+6 ohm
1.00e+6 ohm
IEC 60093
Descriptive Properties Value Comments
Additives Plasticizer
Automotive Fuel systems
Electricals & Electronics Cables & Tubes
Form Granules
Industry & Consumer goods Hydraulics & Pneumatics
Processing Other Extrusion
Product Attributes Flexible
High viscosity
Special Characteristics Anti-static
High impact or impact modified
Improved heat resistance
Improved UV resistance (outdoor use)
Users viewing this material also viewed the following:
Copyright © lookpolymers.com All Rights Reserved