Polymer Property : Tensile Modulus = 50000 ksi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Modulus 345 GPa
50000 ksi
PSM Industries PolyAlloys WNF-3515 Tungsten Heavy Alloy
Mil. T-21014 Class 3, SAE-AMS-T-21014 Class 3, ASTM-B-777-87 Class 3Information Provided by PolyAlloys, a division of PSM Industries
Tensile Modulus 345 GPa
50000 ksi
Young's; DINV ENV 843-2
CeramTec SL 303 Silicon Nitride, SiAION+SiC
SL 303 is a silicon nitride ceramic. Silicon nitrides are ideal for components working under mechanical loads and engine parts, even and especially at elevated temperatures. Their property profile i..