Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 3.51 GPa | 509 ksi | 5 mm/min; ASTM D638 |
SABIC Innovative Plastics Cycoloy® C7210A PC+ABS (Asia Pacific) Cycoloy* C7210A resin is talc-filled PC+ABS, nonhalogenated FR for thinwall molding applications. Very good modulus-ductility balance. |
|||
Tensile Modulus | 3.51 GPa | 509 ksi | 5 mm/min; ASTM D638 |
SABIC Innovative Plastics EXTEM VH1003 PEI Copolymer Transparent, Thermoplastic Polyimide (TPI) resin with a glass transition temperature (Tg) of 247C. This product has thinwall FR capability and has a UL94 V0 listing. This material is RoHS compliant.. |
|||
Tensile Modulus | 3.51 GPa | 509 ksi | 5 mm/min; ASTM D638 |
SABIC Innovative Plastics EXTEM VH1003 PEI Copolymer (Asia Pacific) Transparent, Thermoplastic Polyimide (TPI) resin. Glass transition Temp. (Tg) of 247°C. This resin has thinwall FR capability and has a UL94 V0 listing. Resin is RoHS compliant and halogen free acc.. |
|||
Tensile Modulus | 3.51 GPa | 509 ksi | 5 mm/min; ASTM D638 |
SABIC Innovative Plastics EXTEM VH1003M PEI Copolymer Transparent, Thermoplastic Polyimide (TPI) resin with a glass transition temperature (Tg) of 247C. Internal mold release. This product has thinwall FR capability and has a UL94 V0 listing. This mate.. |
|||
Tensile Modulus | 3.51 GPa | 509 ksi | 5 mm/min; ASTM D638 |
SABIC Innovative Plastics EXTEM VH1003M PEI Copolymer (Asia Pacific) Transparent, Thermoplastic Polyimide (TPI) resin with a glass transition temperature (Tg) of 247C. Internal mold release. This product has thinwall FR capability and has a UL94 V0 listing. This mate.. |
|||
Tensile Modulus | 3.51 GPa | 509 ksi | 5 mm/min; ASTM D638 |
SABIC Innovative Plastics EXTEM VH1003M PEI Copolymer (Europe-Africa-Middle East) Transparent, Thermoplastic Polyimide (TPI) resin. Glass transition Temp. (Tg) of 247°C. Internal mold release. This resin has thinwall FR capability and has a UL94 V0 listing. Resin is halogen free.. |
|||
Tensile Modulus | 3.51 GPa | 509 ksi | 5 mm/min; ASTM D638 |
SABIC Innovative Plastics EXTEM VH1003P PEI Copolymer Transparent, Thermoplastic Polyimide (TPI) resin with a glass transition temperature (Tg) of 247C. Powder version of VH1003. This resin is a Dual-use item and is subject to export control restrictio.. |
|||
Tensile Modulus | 3.51 GPa | 509 ksi | 5 mm/min; ASTM D638 |
SABIC Innovative Plastics EXTEM VH1003P PEI Copolymer (Europe-Africa-Middle East) Transparent, Thermoplastic Polyimide (TPI) resin with a glass transition temperature (Tg) of 247C. Powder version of VH1003. This resin is a Dual-use item and is subject to export control restrictio.. |
|||
Tensile Modulus | 3.51 GPa | 509 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics Lexan® BFL2010 PC Non-brominated, non-chlorinated flame retardant, glass reinforced PC with improved flow. Available in opaque colors. |
|||
Tensile Modulus | 3.51 GPa | 509 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics Lexan® BFL2010 PC (Asia Pacific) Non-brominated, non-chlorinated flame retardant, glass reinforced PC with improved flow. Available in opaque colors. |
|||
Tensile Modulus | 3.51 GPa | 509 ksi | 5 mm/min; ASTM D638 |
SABIC Innovative Plastics EXTEM VH1003F PEI Copolymer (Asia Pacific) Transparent, Thermoplastic Polyimide (TPI) resin. Glass transition Temp. (Tg) of 247°C. Global Food Contact Approval. Resin is subject to Commerce Control Laws U.S. 15CFR Chapter VII, Part 774 and .. |
|||
Tensile Modulus | 3.51 GPa | 509 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics Lexan® BFL2010 PC (Europe-Africa-Middle East) Non-brominated, non-chlorinated flame retardant, glass reinforced PC with improved flow. Available in opaque colors. |
|||
Tensile Modulus | 3.51 GPa | 509 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics LNP LUBRICOMP RAL22I PA 66 LNP* LUBRICOMP* RAL22I is a compound based on Nylon 66 resin containing 10% PTFE, 10% Aramid Fiber. Added features of this material include: Wear Resistant, High Impact. |
|||
Tensile Modulus | 3.51 GPa | 509 ksi | 5 mm/min; ASTM D638 |
SABIC Innovative Plastics ULTEM AUT230 PEI (Europe-Africa-Middle East) Transparent polyetherimide (Tg 247 degC). Very low outgassing and plateout, for automotive lighting applications where highly metallized, reflective surfaces are required. Haze onset temperature of.. |
|||
Tensile Modulus | 3.51 GPa | 509 ksi | 5 mm/min; ASTM D 638 |
SABIC Innovative Plastics Ultem AUT230M PEI Transparent polyetherimide (Tg 247 degC). Contains low level of mold release. Very low outgassing and plateout, for automotive lighting applications where highly metallized, reflective surfaces are .. |
|||
Tensile Modulus | 3.51 GPa | 509 ksi | 5 mm/min; ASTM D 638 |
SABIC Innovative Plastics Ultem AUT230M PEI (Asia Pacific) Transparent polyetherimide (Tg 247 degC) with internal mold release. Very low outgassing and plateout for automotive lighting applications where highly metallized, reflective surfaces are required... |
|||
Tensile Modulus | 3.51 GPa | 509 ksi | 5 mm/min; ASTM D 638 |
SABIC Innovative Plastics Ultem AUT230M PEI (Europe-Africa-Middle East) Transparent polyetherimide (Tg 247 degC) with internal mold release. Very low outgassing and plateout for automotive lighting applications where highly metallized, reflective surfaces are required... |
|||
Tensile Modulus | 3.51 GPa | 509 ksi | 5 mm/min; ASTM D638 |
SABIC Innovative Plastics ULTEM XH6050 PEI Copolymer (Asia Pacific) Transparent, enhanced flow Polyetherimidesulfone copolymer (Tg 247C). ECO Conforming, UL94 V0 listing. Resin is subject to U.S. Commerce Control Laws (15CFR Chapter VII, Part 774). |
|||
Tensile Modulus | 3.51 GPa | 509 ksi | 5 mm/min; ASTM D638 |
SABIC Innovative Plastics ULTEM XH6050F PEI Copolymer Transparent, enhanced flow Polyetherimidesulfone copolymer (Tg 247C). ECO Conforming. US FDA Compliant. Resin is subject to U.S. Commerce Control Laws (15CFR Chapter VII, Part 774). |
|||
Tensile Modulus | 3.51 GPa | 509 ksi | 5 mm/min; ASTM D638 |
SABIC Innovative Plastics ULTEM XH6050F PEI Copolymer (Asia Pacific) Transparent, enhanced flow Polyetherimidesulfone copolymer (Tg 247C). ECO Conforming. US FDA Compliant. Resin is subject to U.S. Commerce Control Laws (15CFR Chapter VII, Part 774). |
|||
Tensile Modulus | 3.51 GPa | 509 ksi | 5 mm/min; ASTM D 638 |
SABIC Innovative Plastics Ultem XH6050F PEI Copolymer (Europe-Africa-Middle East) Transparent, enhanced flow Polyetherimidesulfone copolymer (Tg 247C). ECO Conforming. US FDA Compliant. Resin is subject to U.S. Commerce Control Laws (15CFR Chapter VII, Part 774).This data was .. |
|||
Tensile Modulus | 3.51 GPa | 509 ksi | 5 mm/min; ASTM D638 |
SABIC Innovative Plastics ULTEM XH6050M PEI Copolymer Enhanced flow Polyetherimidesulfone copolymer (Tg 247C) with internal mold release. ECO Conforming, UL94 V0 listing. Resin is subject to U.S. Commerce Control Laws (15CFR Chapter VII, Part 774). |
|||
Tensile Modulus | 3.51 GPa | 509 ksi | 5 mm/min; ASTM D638 |
SABIC Innovative Plastics Valox® 4521 PBT VALOX 4521 is a high flow, 20% glass reinforced flame retardant PBT injection moulding resin. Applications: electrical applications |
|||
Tensile Modulus | 3.51 GPa | 509 ksi | 5 mm/min; ASTM D638 |
SABIC Innovative Plastics Valox® 4521 PBT (Asia Pacific) 19.5% glass reinforced PBT. High flow, flame retardant. |
|||
Tensile Modulus | 3.51 GPa | 509 ksi | 5 mm/min; ASTM D638 |
SABIC Innovative Plastics LNP THERMOCOMP Cycoloy_C7210A PC+ABS LNP* Thermocomp* Cycoloy_C7210A isa a talc-filled PC+ABS, nonhalogenated FR for thinwall molding applications. Very good modulus-ductility balance. |
|||
Tensile Modulus | 3.51 GPa | 509 ksi | 5 mm/min; ASTM D638 |
SABIC Innovative Plastics ULTEM AUT230 PEI Transparent polyetherimide (Tg 247 degC). Very low outgassing and plateout, for automotive lighting applications where highly metallized, reflective surfaces are required. Haze onset temperature of.. |
|||
Tensile Modulus | 3.51 GPa | 509 ksi | 5 mm/min; ASTM D638 |
SABIC Innovative Plastics ULTEM AUT230 PEI (Asia Pacific) Transparent polyetherimide (Tg 247 degC). Very low outgassing and plateout, for automotive lighting applications where highly metallized, reflective surfaces are required. Haze onset temperature of.. |
|||
Tensile Modulus | 3.51 GPa | 509 ksi | 5 mm/min; ASTM D638 |
SABIC Innovative Plastics ULTEM XH6050M PEI Copolymer (Asia Pacific) Enhanced flow Polyetherimidesulfone copolymer (Tg 247C) with internal mold release. ECO Conforming, UL94 V0 listing. Resin is subject to U.S. Commerce Control Laws (15CFR Chapter VII, Part 774). |
|||
Tensile Modulus | 3.51 GPa | 509 ksi | 5 mm/min; ASTM D 638 |
SABIC Innovative Plastics LNP Thermocomp Cycoloy_C7210A PC+ABS (Asia Pacific) Talc-filled PC+ABS, nonhalogenated FR for thinwall molding applications. Very good modulus-ductility balance.This data was supplied by SABIC-IP for the Asia Pacific region. |
|||
Tensile Modulus | 3.51 GPa | 509 ksi | 1 mm/min |
Arkema Group Orgalloy® RS 6015 BV Nylon 6 Alloy, Glass Fiber + Bead Filled (Conditioned) RS 60 series, rigid polyamide 6 alloy: easy to process, chemical resistance (no known solvents) and low moisture absorption leading to stability of mechanical, electrical and dimensional properties.. |