Tensile Modulus 3.699 GPa
536.5 ksi
ASTM D638
Aclo Accutech Nylon 6 NY0730G20L Glass Reinforced
Tensile Modulus 3.699 GPa
536.5 ksi
ASTM D638
Aclo Accutech Polyethylene HD0234G30UVL High Density Glass Reinforced UV Stabilized
Tensile Modulus 3.699 GPa
536.5 ksi
ASTM D638
Aclo Accutech Polypropylene Homopolymer HP0336G15M15CL Glass/Mineral Reinforced Coupled
Tensile Modulus 3.699 GPa
536.5 ksi
ASTM D638
Aclo Accutech Polypropylene Homopolymer HP0336G20M10CL Glass/Mineral Reinforced Coupled
Tensile Modulus 3.699 GPa
536.5 ksi
ASTM D638
Aclo Accutech Polypropylene Homopolymer HP0336M30CL Mica Reinforced Coupled
Tensile Modulus 3.699 GPa
536.5 ksi
ASTM D638
Aclo Accutech Polypropylene Homopolymer HP0339G15M15CL Glass/Mineral Reinforced Coupled
Tensile Modulus 3.699 GPa
536.5 ksi
ASTM D638
Aclo Accutech Polypropylene Homopolymer HP0339G25M5CL Glass/Mineral Reinforced Coupled