Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Aclo Accutech Polypropylene Homopolymer HP0336G20M10CL Glass/Mineral Reinforced Coupled

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene, Glass/Mineral Reinforced
Manufacturer Aclo Compounders
Trade Name Accutech
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Aclo Accutech Polypropylene Homopolymer HP0336G20M10CL Glass/Mineral Reinforced Coupled.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Physical Properties Metric English Comments
Density 1.11 g/cc
0.0401 lb/in³
ASTM D792
Linear Mold Shrinkage 0.0020 cm/cm
0.0020 in/in
MD; ASTM D955
Melt Flow 3.0 g/10 min
3.0 g/10 min
ASTM D1238
Ash 30 %
30 %
ASTM D2584
Mechanical Properties Metric English Comments
Hardness, Rockwell R 92
92
ASTM D785
Tensile Strength at Break 56.0 MPa
8120 psi
ASTM D638
Tensile Strength, Yield 57.0 MPa
8270 psi
ASTM D638
Elongation at Break 6.0 %
6.0 %
ASTM D638
Elongation at Yield 4.0 %
4.0 %
ASTM D638
Tensile Modulus 3.699 GPa
536.5 ksi
ASTM D638
Flexural Strength 85.98 MPa
12470 psi
ASTM D790
Flexural Modulus 4.799 GPa
696.1 ksi
ASTM D790
Izod Impact, Notched 0.641 J/cm
1.20 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 154 °C
309 °F
ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 133 °C
271 °F