Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 3.70 GPa | 537 ksi | |
Plastcom SLOVASTER® B1 GF 6/2 PBT reinforced with 6% glass fibre Features: PBT for injection moulding, chemically reinforced with 6 % glass fibre. Characterised by excellent properties also at minus temperatures like eg. modulus of elasticity in tension and bendi.. |
|||
Tensile Modulus | 3.70 GPa | 537 ksi | 50 mm/min; ASTM D638 |
Ovation Polymers Nima™ NH OPP66GF25 FR 25% Glass Filled Polyamide 66 Non-Hal red phosphorous based Flame Retardant CompoundAll properties after 48hrs conditioning at 23°C/50% RH |
|||
Tensile Modulus | 3.70 GPa @Temperature 23.0 °C |
537 ksi @Temperature 73.4 °F |
ISO 527-2/1 |
PolyOne Bergamid™ B700 Mi10 UF Polyamide 6 (Nylon 6) Information provided by PolyOne |
|||
Tensile Modulus | 3.70 GPa | 537 ksi | 50 mm/min; ASTM D638 |
Solvay Specialty Polymers AvaSpire® AV-722 Polyaryletherketone (PAEK)
(Unverified Data**) AvaSpire AV-722 is an unreinforced polyaryletherketone (PAEK) that offers improved economics relative to PEEK while retaining most of PEEK's key performance attributes. AV-722 resin has been formula.. |
|||
Tensile Modulus | 3.70 GPa | 537 ksi | 1.0 mm/min; ASTM D638 |
Solvay Specialty Polymers KetaSpire® KT-880 Polyetheretherketone (PEEK)
(Unverified Data**) KetaSpire KT-880 is a high flow grade of unreinforced polyetheretherketone (PEEK) supplied in pellet form. KetaSpire PEEK is produced to the highest industry standards and is characterized by a dist.. |
|||
Tensile Modulus | 3.70 GPa | 537 ksi | 5 mm/min; ASTM D638 |
SABIC Innovative Plastics Lexan® HFD4271 PC Lexan* HFD4271 is a 10% glass filled, high flow, impact modified, injection moldable grade designed for high flow and superior surface appearance. HFD4271 has enhanced mold release, impact ductility.. |
|||
Tensile Modulus | 3.70 GPa | 537 ksi | 5 mm/min; ASTM D638 |
SABIC Innovative Plastics Lexan® HFD4271 PC (Asia Pacific) Lexan* HFD4271 is a 10% glass filled, high flow, impact modified, injection moldable grade designed for high flow and superior surface appearance. HFD4271 has enhanced mold release, impact ductility.. |
|||
Tensile Modulus | 3.70 GPa | 537 ksi | |
LATI Latistat 66-06 PA66 Dissipative product based on Polyamide 66 (PA66). Unfilled. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industria Termoplastici.. |
|||
Tensile Modulus | 3.70 GPa | 537 ksi | DIN 53457 |
Schwartz Technical Plastics LAMIGAMID® 310 Cast Polyamide 6, Dry Application: sheaves, wheels, rollers, mandrell segments, coupling parts, vibrator parts etc.Information provided by Schwartz Technical Plastics GmbH |
|||
Tensile Modulus | 3.70 GPa | 537 ksi | ASTM D638 |
Solvay Specialty Polymers KetaSpire® KT-880 NL Polyetheretherketone (PEEK) KetaSpire® KT-880 NL is a high flow grade of unreinforced polyetheretherketone (PEEK) supplied in non-lubricated, natural-color pellet form. KetaSpire® PEEK is produced to the highest industry.. |
|||
Tensile Modulus | 3.70 GPa | 537 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics Valox® 745 PBT (Europe-Africa-Middle East) VALOX 745 is 30% mineral filled PBT injection moulding resin with improved toughness and low warpage. Applications: telephone ringer frames, card racks. |
|||
Tensile Modulus | 3.70 GPa | 537 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics LNP THERMOCOMP DZ004 PC (Asia Pacific) LNP* Thermocomp* DZ004 is a compound based on Polycarbonate resin containing Glass Fiber. Also known as Thermocomp DF-1004 M |
|||
Tensile Modulus | 3.70 GPa | 537 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP Thermocomp KB005 Acetal Copolymer LNP THERMOCOMP* KB005 is a compound based on Acetal Copolymer resin containing Glass Bead.This data was supplied by SABIC-IP for the Americas region. |
|||
Tensile Modulus | 3.70 GPa @Temperature 23.0 °C |
537 ksi @Temperature 73.4 °F |
|
Hexcel® HexPly® 954-6 Curing Cyanate Resin HexPly® 954-6 is a 250°F (121°C) curing toughened cyanate resin with 300°F (149°C) Tg. HexPly® 954-6 is formulated for autoclave curing. Recommended cure is three hours at 250°F (121°C). Ser.. |
|||
Tensile Modulus | 3.70 GPa | 537 ksi | ISO 527-1, 2 |
Polyplastics Duracon® TR-10D Acetal Co-polymer (POM), Mineral filling, Mineral filling, High rigidity, Low warpage DURACON® is a crystalline thermoplastic acetal copolymer. The primary raw material trioxane, a trimer of formaldehyde.The thermoplastic adopts a copolymer structure in which polyoxymethylene (-C-O).. |
|||
Tensile Modulus | 3.70 GPa | 537 ksi | ASTM D 638 |
Cossa Polimeri ESTAPROP K 1280 T8 Polypropylene, 40% Mineral Filled PP copolymer 40% mineral fillerExcellent physical and mechanical characteristics, good surface appearanceInformation provided by Cossa Polimeri S.r.l. |
|||
Tensile Modulus | 3.70 GPa | 537 ksi | dry; ISO 527-1/-2 |
DSM Akulon® K224-PG2 PA6-I-GF8 8% Glass Reinforced, Impact Modified |
|||
Tensile Modulus | 3.70 GPa @Temperature 23.0 °C |
537 ksi @Temperature 73.4 °F |
EN ISO 527 |
Ensinger TECASINT™ 2011 Polyimide (PI) TECASINT™ 2000 series of polyimide stock shapes provide a superior combination of high temperature and bearing and wear, properties that make it an ideal choice for the most demanding applications... |
|||
Tensile Modulus | 3.70 GPa | 537 ksi | 1 mm/min; ISO 527 |
Eurostar Staramide AS3 PA66, 15% Glass Bead Reinforced, Injection Molding Staramide AS3 is a 15% Glass Bead Reinforced Polyamide 66, Injection Molding ResinInformation provided by Eurostar. |
|||
Tensile Modulus | 3.70 GPa | 537 ksi | ISO 527 |
Cossa Polimeri ESTABLEND PA 2516 GF ABS / Nylon 6 Blend, 8% Glass Filled ESTABLEND PA is a blend of acrylonitrile butadiene styrene and polyamide 6.8% glass fiber reinforcedExceptional chemical resistance, excellent heat resistance, good dimensional stabilityInformation .. |
|||
Tensile Modulus | 3.70 GPa | 537 ksi | dry; ISO 527-1/-2 |
EMS-Grivory Grivory® BS V0 PA6 Product description: Grilon BS V0 is an unreinforced, normal viscosity, self-extinguishing PA6 injection molding grade. Grilon BS V0 has the following important properties: Halogen and phosphorous-f.. |
|||
Tensile Modulus | 3.70 GPa | 537 ksi | dry; ISO 527 |
Azoty Tarnow™ Tarnamid® T-27 MCS V0 Polyamide 6 - Flame Retarded, Unreinforced Flame retarded (class V0), bromine and red phosphorus free, medium viscosity injection molding grade, also used for compounding, for production of monofilament, bristles and fibers.Tarnamid® has th.. |
|||
Tensile Modulus | 3.70 GPa | 537 ksi | 1[mm/min]; ISO 527-1/2 |
Akro-Plastic Akromid® A3 GF 15 (2418) PA 6.6 Conditioned, 15% Glass Filled AKROMID® A (Polyamide 6.6) is an engineering compound, characterized by high mechanical strength, stiffness and thermal resistance. Furthermore, this polyamide offers high toughness at low temperat.. |
|||
Tensile Modulus | 3.70 GPa | 537 ksi | same value from ASTM and ISO test. |
BASF Capron® 5202CQ Blend HS Blend Nylon 66 (Dry)
(discontinued **) Capron 5202CQ HS Blend is a heat stabilized, blended polyamide 6,6 injection molding homopolymer developed for fast molding cycles. It is also available in pigmented versions.Capron 5202CQ HS Blend.. |
|||
Tensile Modulus | 3.70 GPa | 537 ksi | 1mm/min; ISO 527 |
Styrolution Luran® 368 R SAN General-purpose grade with well-balanced properties intended for both injection molding and extrusion.Information provided by STYROLUTION, which is a joint venture between BASF and INEOS. |
|||
Tensile Modulus | 3.70 GPa | 537 ksi | ISO 527 |
Victrex® HT™ G45 Polyetherketone Product Description: High performance thermoplastic material, unreinforced PolyEtherKetone (PEK), semi crystalline, depth filtered granules for injection moulding, low flow, FDA food contact complia.. |
|||
Tensile Modulus | 3.70 GPa @Temperature 23.0 °C |
537 ksi @Temperature 73.4 °F |
ISO 527 |
Victrex® PEEK 380P Polyetheretherketone, Unreinforced Product Description:High performance thermoplastic material, unreinforced Polyetheretherketone (PEEK), semi crystalline, coarse powder for extrusion compounding, medium flow, FDA food contact compli.. |
|||
Tensile Modulus | 3.70 GPa | 537 ksi | 5 mm/min; ASTM D638 |
SABIC Innovative Plastics Lexan® HFD4471 PC (Asia Pacific) Lexan* HFD4471 is a 10% glass filled, medium flow, impact modified, injection moldable grade designed for high flow and superior surface appearance. HFD4417 has enhanced mold release, impact ductili.. |