Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Plastcom SLOVASTER® B1 GF 6/2 PBT reinforced with 6% glass fibre

Category Polymer , Thermoplastic , Polyester, TP , Polybutylene Terephthalate (PBT) , Polybutylene Terephthalate (PBT), 10% Glass Fiber Filled
Manufacturer Plastcom spol. s r.o.
Trade Name SLOVASTER®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Plastcom SLOVASTER® B1 GF 6/2 PBT reinforced with 6% glass fibre.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Features: PBT for injection moulding, chemically reinforced with 6 % glass fibre. Characterised by excellent properties also at minus temperatures like eg. modulus of elasticity in tension and bending, tensial strength, toughness. Does not absorb water, that means that identical properties are maintained also in wet environment. Melt is characterised by very good rheology, which enables manufacturing of extremely multiple products with complicated downflow-path. Anisotropy of shrinkage is much better in comparison with PA, what influences themanufacturing of round, cylindric or other hole products. Application in the automotive, electrical and engineering industry - connectors of cable harnesses, car-door locks, connection links, grips etc. Delivered in natural mode and in the full RAL colour scale.Packaging, transport, stocking: The product is packed in hermetically closed thick-walled 25 kg PE bags, on a 1.000 kg palette coated in a stretch foil, in big bags with a thick PE foil fixed on a 1.000 kg palette, in paper octabins with a thick PE foil fixed on a 1.000 kg palette or in other packaging according to customer requirements. The transport is provided in closed-up vehicles where the material is protected against movement and mechanical damage. The product requires stocking in closed-up, dry places protected against sun and thermal radiation.Information Provided by Plastcom spol. s r.o.
Physical Properties Metric English Comments
Density 1.35 g/cc
0.0488 lb/in³
Linear Mold Shrinkage 0.0090 cm/cm
0.0090 in/in
Linear Mold Shrinkage, Transverse 0.011 cm/cm
0.011 in/in
Melt Flow 25 g/10 min

@Load 2.16 kg,
Temperature 250 °C
25 g/10 min

@Load 4.76 lb,
Temperature 482 °F
Mechanical Properties Metric English Comments
Tensile Strength at Break 70.0 MPa
10200 psi
Elongation at Break 7.0 %
7.0 %
Tensile Modulus 3.70 GPa
537 ksi
Flexural Strength 105 MPa
15200 psi
Flexural Modulus 2.85 GPa
413 ksi
Charpy Impact Unnotched 3.00 J/cm²

@Temperature 23.0 °C
14.3 ft-lb/in²

@Temperature 73.4 °F
3.00 J/cm²

@Temperature -20.0 °C
14.3 ft-lb/in²

@Temperature -4.00 °F
Charpy Impact, Notched 0.400 J/cm²

@Temperature 23.0 °C
1.90 ft-lb/in²

@Temperature 73.4 °F
0.400 J/cm²

@Temperature -20.0 °C
1.90 ft-lb/in²

@Temperature -4.00 °F
Thermal Properties Metric English Comments
Melting Point 223 °C
433 °F
Deflection Temperature at 1.8 MPa (264 psi) 200 °C
392 °F
Vicat Softening Point 205 °C
401 °F
Flammability Test 1.0
1.0
Glow Wire Test 750 °C
1380 °F
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+13 ohm-cm
1.00e+13 ohm-cm
Surface Resistance 1.00e+13 ohm
1.00e+13 ohm
Dielectric Strength 23.0 kV/mm
584 kV/in
Comparative Tracking Index 300 V
300 V
Processing Properties Metric English Comments
Melt Temperature 240 - 260 °C
464 - 500 °F
Mold Temperature 50.0 - 80.0 °C
122 - 176 °F
Drying Temperature 120 °C
248 °F
Dry Time 4 hour
4 hour
Moisture Content 0.050 %
0.050 %
Injection Pressure 60.0 - 100 MPa
8700 - 14500 psi
Users viewing this material also viewed the following: