Mechanical Properties Metric English Comments
Tensile Modulus 3.86 GPa
560 ksi
5 mm/min; ASTM D 638
SABIC Innovative Plastics Cycolac® INP563 ABS
SABIC INP563 provides compatibility with a wider range of ABS grades than many color concentrate bases; allows better dispersion than pellets; allows concentrate manufacturers to produce both pellet..
Tensile Modulus 3.86 GPa
560 ksi
5 mm/min; ASTM D638
SABIC Innovative Plastics Cycolac® INP563 ABS+SAN
SABIC INP563 provides compatibility with a wider range of ABS grades than many color concentrate bases; allows better dispersion than pellets; allows concentrate manufacturers to produce both pellet..
Tensile Modulus 3.86 GPa
560 ksi
ASTM D638
Fiberfil® PP-60/TC/40 Polypropylene Homopolymer, 40% Talc Filled
Information provided by FIBERFIL Engineered Plastics
Tensile Modulus 3.86 GPa
560 ksi
1 mm/min; ISO 527
SABIC Innovative Plastics Xenoy® X6320 PBT+PC (Asia Pacific)
X6320 is a mineral filled PBT/PC resin developed for automotive painted doorhandles. Key advantages are excellent surface finish, easy processing and paint quality.
Tensile Modulus 3.86 GPa
560 ksi
1 mm/min; ISO 527
SABIC Innovative Plastics Xenoy® X6320 PBT+PC
X6320 is a mineral filled PBT/PC resin developed for automotive painted doorhandles. Key advantages are excellent surface finish, easy processing and paint quality.This data was supplied by SABIC-IP..