Polymer Property : Tensile Modulus = 6.13 GPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Modulus 6.13 GPa
889 ksi
1 mm/min; ISO 527
SABIC Innovative Plastics LNP LUBRICOMP BX03658N SAN
LNP* LUBRICOMP* BX03658N is a compound based on SAN resin containing proprietary fillers. Added features of this grade include: Wear Resistant, Tight Dimensional Tolerances, good for Water Meter A..
Tensile Modulus 6.13 GPa
889 ksi
50 mm/min; ASTM D638
SABIC Innovative Plastics LNP LUBRICOMP KZL16 Acetal Copolymer
LNP LUBRICOMP* KZL16 is a compound based on Acetal Copolymer resin containing Glass Fiber, Milled Glass, PTFE. Added features of this material include: Internally Lubricated.
Tensile Modulus 6.13 GPa
889 ksi
ISO 527 Type 1A
Solvay TECHNYL® 52G1MX 25 Grey 7035 PA6, DRY
Description: Flame retardant polyamide PA6 reinforced with mineral filler for injection molding, also suitable for thin wall parts.Available in: Asia Pacific, Europe, Latin America and North America..
Tensile Modulus 6.13 GPa
889 ksi
1mm/min; ISO 527
BASF Ultramid® 8231G HS BK-102 14% Glass Filled PA6 (Dry)
Ultramid 8231G HS BK-102 is a black pigmented heat stabilized, 14% glass fiber reinforced PA6 injection molding compound.The glass fiber reinforcement enhances performance such as strength, stiffnes..