Polymer Property : Tensile Modulus = 6.29 GPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Modulus 6.29 GPa
912 ksi
Clear Casting
TSE Industries EcoSPRAY® 350c Flame-Retardant Polyurethane Resin
TSE-EcoSPRAY® 350c is an “Environmentally-Preferred Product” or EPP. It is a Thixotropic flame retardant polyurethane resin free of Styrene, and is an “ultra-low” emitting resin during applica..
Tensile Modulus 6.29 GPa
912 ksi
1 mm/min; ISO 527
SABIC Innovative Plastics LNP THERMOCOMP MC002 PP
LNP* THERMOCOMP* MC002 is a compound based on Polypropylene resin containing 10% Carbon Fiber. Added feature of this material is: Electrically Conductive.
Tensile Modulus 6.29 GPa
912 ksi
Clear Casting
TSE Industries EcoSPRAY® 350c Flame-Retardant Polyurethane Resin
TSE-EcoSPRAY® 350c is an “Environmentally-Preferred Product” or EPP. It is a Thixotropic flame retardant polyurethane resin free of Styrene, and is an “ultra-low” emitting resin during applica..