Mechanical Properties Metric English Comments
Tensile Modulus 6.37 GPa
925 ksi
5 mm/min; ASTM D638
Samsung Cheil Industries Infino® HM-3301GL PC, Glass Filled High Impact
PC/GF material that is used for electric and electronic partsInformation provided by Samsung Cheil Industries.
Tensile Modulus 6.37 GPa
924 ksi
50 mm/min; ASTM D638
SABIC Innovative Plastics LNP THERMOCOMP QF004 PA 6/10
LNP* THERMOCOMP* QF004 is a compound based on Nylon 6/10 resin containing 20% Glass Fiber.
Tensile Modulus 6.37 GPa
924 ksi
50 mm/min; ASTM D638
SABIC Innovative Plastics LNP THERMOCOMP QF004 PA 6/10 (Asia Pacific)
LNP* Thermocomp* QF004 is a compound based on Nylon 6/10 resin containing Glass Fiber.
Tensile Modulus 6.37 GPa
924 ksi
1 mm/min; ISO 527
SABIC Innovative Plastics LNP THERMOCOMP RF0029S PA 66
LNP* THERMOCOMP* RF0029S is a compound based on Nylon 66 resin containing 10% Glass Fiber. Added features of this material include: Flame Retardant, Heat Stabilized.
Tensile Modulus 6.37 GPa
924 ksi
1 mm/min; ISO 527
SABIC Innovative Plastics LNP THERMOCOMP RF0029S PA 66 (Asia Pacific)
LNP* Thermocomp* RF0029S is a compound based on Nylon 66 resin containing Glass Fiber, Flame Retardant. Added features of this material include: Flame Retardant, Heat Stabilized.
Tensile Modulus 6.37 GPa

@Temperature -40.0 °C
924 ksi

@Temperature -40.0 °F
ISO Data
BASF Ultramid® 8272G HS BK-102 12% Glass Filled PA6 (Dry)
Ultramid 8272G HS BK-102 is a 12% glass fiber reinforced, black pigmented, thermally modified, nylon 6 blow molding compound offering an excellent balance of engineering properties combined with the..
Tensile Modulus 6.37 GPa
925 ksi
5 mm/min; ASTM D638
Samsung Cheil Industries Infino® HM-3301GL PC, Glass Filled High Impact
PC/GF material that is used for electric and electronic partsInformation provided by Samsung Cheil Industries.
Copyright © lookpolymers.com All Rights Reserved