Polymer Property : Tensile Modulus = 6.42 GPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Modulus 6.42 GPa
931 ksi
1 mm/min; ISO 527
SABIC Innovative Plastics LNP LUBRICOMP UX06425 PPA
LNP* LUBRICOMP* UX06425 is a compound based on Polyphthalamide (PPA) containing 10% Glass Fiber, 10% PTFE. Added features of this material include: Wear Resistant, Hot Water Moldable and Heat Stab..