Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

SABIC Innovative Plastics LNP LUBRICOMP UX06425 PPA

Category Polymer , Thermoplastic , Polyphthalamide (PPA)
Manufacturer SABIC Innovative Plastics (GE Plastics)
Trade Name LNP LUBRICOMP
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF SABIC Innovative Plastics LNP LUBRICOMP UX06425 PPA.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
LNP* LUBRICOMP* UX06425 is a compound based on Polyphthalamide (PPA) containing 10% Glass Fiber, 10% PTFE. Added features of this material include: Wear Resistant, Hot Water Moldable and Heat Stabilized.
Physical Properties Metric English Comments
Specific Gravity 1.34 g/cc
1.34 g/cc
ASTM D792
Density 1.33 g/cc
0.0480 lb/in³
ASTM D792
Moisture Absorption 0.310 %
0.310 %
50% RH, 24 hrs; ASTM D570
0.500 %
0.500 %
23°C / 50% RH; ISO 62
Linear Mold Shrinkage, Flow 0.0070 - 0.0090 cm/cm

@Time 86400 sec
0.0070 - 0.0090 in/in

@Time 24.0 hour
ASTM D955
Linear Mold Shrinkage, Transverse 0.010 - 0.030 cm/cm

@Time 86400 sec
0.010 - 0.030 in/in

@Time 24.0 hour
ASTM D955
Mechanical Properties Metric English Comments
Tensile Strength at Break 85.0 MPa
12300 psi
5 mm/min; ISO 527
89.0 MPa
12900 psi
Type I, 5 mm/min; ASTM D638
Elongation at Break 1.4 %
1.4 %
5 mm/min; ISO 527
1.5 %
1.5 %
Type I, 5 mm/min; ASTM D638
Elongation at Yield 1.4 %
1.4 %
5 mm/min; ISO 527
Tensile Modulus 6.42 GPa
931 ksi
1 mm/min; ISO 527
6.61 GPa
959 ksi
50 mm/min; ASTM D638
Flexural Strength 126 MPa
18300 psi
ISO 178
132 MPa
19100 psi
1.3 mm/min, 50 mm span; ASTM D790
Flexural Modulus 5.44 GPa
789 ksi
2 mm/min; ISO 178
5.71 GPa
828 ksi
1.3 mm/min, 50 mm span; ASTM D790
Izod Impact, Notched 0.330 J/cm
0.618 ft-lb/in
ASTM D256
Izod Impact, Unnotched 1.97 J/cm
3.69 ft-lb/in
ASTM D4812
Izod Impact, Notched (ISO) 3.00 kJ/m²
1.43 ft-lb/in²
80*10*4; ISO 180/1A
Izod Impact, Unnotched (ISO) 12.0 kJ/m²
5.71 ft-lb/in²
80*10*4; ISO 180/1U
Dart Drop, Total Energy 3.00 J

@Temperature 23.0 °C
2.21 ft-lb

@Temperature 73.4 °F
ASTM D3763
Impact Test 1.00 J
0.738 ft-lb
Multiaxial Impact; ISO 6603
Coefficient of Friction, Dynamic 0.36
0.36
ASTM D3702 Modified
Coefficient of Friction, Static 0.37
0.37
ASTM D3702 Modified
K (wear) Factor 30.2 x 10-8 mm³/N-M
15.0 x 10-10 in³-min/ft-lb-hr
Washer; ASTM D3702 Modified
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 41.0 µm/m-°C

@Temperature -30.0 - 30.0 °C
22.8 µin/in-°F

@Temperature -22.0 - 86.0 °F
ASTM D696
CTE, linear, Transverse to Flow 75.0 µm/m-°C

@Temperature -30.0 - 30.0 °C
41.7 µin/in-°F

@Temperature -22.0 - 86.0 °F
ASTM D696
Deflection Temperature at 0.46 MPa (66 psi) 289 °C
552 °F
Flatw 80*10*4 sp=64mm; ISO 75/Bf
293 °C

@Thickness 3.20 mm
559 °F

@Thickness 0.126 in
unannealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 254 °C
489 °F
Flatw 80*10*4 sp=64mm; ISO 75/Af
260 °C

@Thickness 3.20 mm
500 °F

@Thickness 0.126 in
unannealed; ASTM D648
Users viewing this material also viewed the following: