Polymer Property : Tensile Modulus = 61.0 GPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Modulus 61.0 GPa
8850 ksi
Goodfellow Cobalt/Silicon/Boron/Iron/Nickel Alloy
Metallic glasses (glassy alloys) or amorphous metals. Uses include soft magnetic applications, brazing, coating and as reinforcing fibers.Information provided by Goodfellow.
Tensile Modulus 61.0 GPa

@Temperature 23.0 °C
8850 ksi

@Temperature 73.4 °F
0°, Conditioning: 23°C; ASTM D3039
Hexcel® HexPly® M49 120°C Curing Epoxy Matrix, AS4-C
Fiber Designation: C193PW, Plain weaveInformation provided by HexCel