Goodfellow Cobalt/Silicon/Boron/Iron/Nickel Alloy

Category Metal , Electronic/Magnetic Alloy , Nonferrous Metal , Cobalt Alloy
Manufacturer Goodfellow
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Goodfellow Cobalt/Silicon/Boron/Iron/Nickel Alloy.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Metallic glasses (glassy alloys) or amorphous metals. Uses include soft magnetic applications, brazing, coating and as reinforcing fibers.Information provided by Goodfellow.
Physical Properties Metric English Comments
Density 7.59 g/cc
0.274 lb/in³
Mechanical Properties Metric English Comments
Vickers Microhardness 960
960
kg(f)/mm²
Tensile Strength at Break >= 700 MPa
>= 102000 psi
Tensile Modulus 61.0 GPa
8850 ksi
Thermal Properties Metric English Comments
Crystallization Temperature 550 °C
1020 °F
Maximum Service Temperature, Air 80.0 °C
176 °F
Component Elements Properties Metric English Comments
Boron, B 14 %
14 %
Cobalt, Co 66 %
66 %
Iron, Fe 4.0 %
4.0 %
Nickel, Ni 1.0 %
1.0 %
Silicon, Si 15 %
15 %
Electrical Properties Metric English Comments
Electrical Resistivity 0.000142 ohm-cm
0.000142 ohm-cm
Magnetic Coercive Force, Hc 0.0030 Oe
0.0030 Oe
Magnetic Saturation Flux Density, Bmax 5500 Gauss
5500 Gauss
Magnetic Remanence, Br 0.82 Gauss
0.82 Gauss
Remanence Ratio, B<sub>r</sub>/B<sub>s</sub>
Curie Temperature 205 °C
401 °F