Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 4.21 GPa | 610 ksi | Type 1 - Rigids, 0.2 in/min; ASTM D638 |
PolyOne Edgetek® PS-25MN/000 Polybutylene Terephthalate (PBT), Mineral Filled
(discontinued **) Description/Features:Mineral FilledUL 94 HBPolyOne First ChoiceInformation provided by PolyOne Corporation. |
|||
Tensile Modulus | 4.20 GPa @Temperature 90.0 °C |
610 ksi @Temperature 194 °F |
Dynamic; ISO 11403-1 -2 |
DuPont Performance Polymers Crastin® SK605 NC010 Polybutylene Terephthalate (PBT)
(Unverified Data**) 30% Glass Reinforced Polybutylene Terephthalate Crastin SK605 NC010 is a 30% glass fiber reinforced lubricated polybutylene terephthalate resin for injection molding.Information provided by DuPont P.. |