Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Tensile Modulus = 66.7 ksi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Modulus 0.460 GPa

@Temperature 120 °C
66.7 ksi

@Temperature 248 °F
DAM; ISO 11403-1 -2
DuPont Performance Polymers Zytel® 101L NC010 Nylon 66  (Unverified Data**)
Unreinforced Polyamide 66Zytel 101L NC010 is a lubricated polyamide 66 resin for injection molding.Information provided by DuPont Performance Polymers
Tensile Modulus 0.460 GPa
66.7 ksi
1 mm/min
Arkema Group Rilsan® 8020 Nylon 11, Flexible Tubing Grade (Dry)
Designation ISO 1874-PA11/xx,E,16-003Transparent and flexible copolymer for tubes extrusion. Additive free.Good flexibility. Very good transparency. High chemical resistance.USP XXIII class VI appro..
Tensile Modulus 0.460 GPa
66.7 ksi
1mm/min; ISO 527
BASF Ultramid® 8254 HS BK-102 PA6 (Conditioned)
Ultramid 8254 HS is a highly flexible, heat stabilized, impact modified nylon 6 extrusion grade for tubing applications.
Tensile Modulus 0.460 GPa
66.7 ksi
1 mm/min
Arkema Group Orgalloy® LT 5050 Flexible Nylon Alloy (Conditioned)
Very flexible polyamide alloy: easy to process, low moisture absorption, good mechanical properties at low temperature. Demonstrate a good balance of properties eg, high flexibility (500 MPa), good ..
Tensile Modulus 0.460 GPa
66.7 ksi
1 mm/min
Arkema Group Orgalloy® LT 5050ES Flexible Nylon Alloy (Conditioned)
Very flexible polyamide alloy: easy to process, low moisture absorption, good mechanical properties at low temperature. Demonstrate a good balance of properties eg, high flexibility (500 MPa), good ..
Tensile Modulus 0.460 GPa
66.7 ksi
1 mm/min
Arkema Group Orgalloy® LT 5050T Flexible Nylon Alloy (Conditioned)
Very flexible polyamide alloy: easy to process, low moisture absorption, good mechanical properties at low temperature. Demonstrate a good balance of properties eg, high flexibility (500 MPa), good ..