Tensile Modulus 7.92 GPa
1150 ksi
50 mm/min; ASTM D638
SABIC Innovative Plastics LNP THERMOCOMP WX88406 Polyester, TP
LNP* Thermocomp* WX88406 is a compound based on Polyester, TP resin.