Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 5.08 GPa | 737 ksi | 50 mm/min; ASTM D 638 |
SABIC Innovative Plastics LNP Lubricomp KFL22 Acetal Copoly (Asia Pacific) LNP* Lubricomp* KFL22 is a compound based on Acetal Copolymer resin containing Glass Fiber, PTFE. Added features of this material include: Internally Lubricated.This data was supplied by SABIC-IP f.. |
|||
Tensile Modulus | 5.08 GPa | 737 ksi | 50 mm/min; ASTM D 638 |
SABIC Innovative Plastics LNP Lubricomp KFL22 Acetal Copolymer LNP* Lubricomp* KFL22 is a compound based on Acetal Copolymer resin containing Glass Fiber, PTFE. Added features of this material include: Internally Lubricated.This data was supplied by SABIC-IP f.. |
|||
Tensile Modulus | 5.08 GPa | 737 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP THERMOCOMP RF002XXH PA 66 LNP THERMOCOMP* RF002XXH is a compound based on Nylon 66 resin containing 10% Glass Fiber. Added feature of this material includes: Healthcare. |