Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 53.0 GPa | 7690 ksi | longitudinal; ISO 527-4/5 |
Bond Laminates TEPEX® dynalite 201-C200(x)/45% Carbon – PA6.6 Consolidated Composite Laminate Within the TEPEX® composite laminate, Polyamide 66 is a resin known for its high hardness, stiffness, abrasion resistance, heat and chemical resistances. The carbon used within this material is ae.. |