Polymer Property : Tensile Modulus = 7830 ksi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Modulus 54.0 GPa

@Temperature 23.0 °C
7830 ksi

@Temperature 73.4 °F
0°, Conditioning: 23°C; ASTM D3039
Hexcel® HexPly® M49 120°C Curing Epoxy Matrix, 6K High Strength Carbon
Fiber Designation: C370S5, Satin weave, 5HInformation provided by HexCel
Tensile Modulus 54.0 GPa
7830 ksi
Warp; EN2597B
Ensinger TECATEC™ CF60 Polyaryletherketone (PAEK)
TECATEC™ CF60 plate is a composite of 60% woven carbon fiber laminated with a polyaryl ether ketone resin (PAEK). It is produced in a proprietary process yielding good fibre and resin integration...