Mechanical Properties Metric English Comments
Tensile Modulus 60.0 GPa
8700 ksi
ASTM D3039
Greene Tweed Orthetek® WF Polyketone, Continuous Woven Carbon Fiber
Greene Tweed offers precision-molded thermoplastic components made from our high-performance Orthtek® composite materials for a variety of demanding medical and biotechnology applications. Ortht..
Tensile Modulus 60.0 GPa
8700 ksi
Greene Tweed Xycomp® 1030-01 Carbon/Nylon 12 Composite
Greene, Tweeds Xycomp® engineered components offer a wider range of benefits than conventional thermoset resin systems because they rely on thermoplastic resins for their matrix. With specific st..
Tensile Modulus 60.0 GPa
8700 ksi
ASTM D3039
Greene Tweed WRâ„¢ 575 PEEK, Bi-Directional Carbon Fiber Filled
WR®575 is a thermoplastic composite consisting of bi-directionally oriented carbon fibers in a PEEK matrix. The excellent wear resistance and the fiber orientation of WR575 makes this material i..
Tensile Modulus 60.0 - 90.0 GPa
8700 - 13100 ksi
Goodfellow Nickel 55/Titanium 45 Shape Memory Alloy
Shape memory alloy is a description applied to that group of metallic materials which show the ability to return to the previously defined shape or size when subjected to the correct thermal procedu..
Tensile Modulus 60.0 GPa

@Temperature 135 °C
8700 ksi

@Temperature 275 °F
90º, Wet; EN2561
Hexcel® HexPly® M42 180°C (350°F) Curing Epoxy Matrix, 50%/G939 HS Carbon
Information provided by HexCel
Tensile Modulus 60.0 GPa

@Temperature 75.0 °C
8700 ksi

@Temperature 167 °F
90º, Wet; EN2561
Hexcel® HexPly® M12 135°C Curing Epoxy Matrix, 45% 46280 Fiber
Information provided by HexCel
Tensile Modulus 60.0 GPa

@Temperature 23.0 °C
8700 ksi

@Temperature 73.4 °F
0º, Conditioning: 23°C; ASTM D3039
Hexcel® HexPly® M47 140°C Curing Epoxy Matrix, Woven Carbon Prepreg
42% resin weight with C193PW(HTA) - 193 g/m2 plain weave 3K HTA 49% fiber volumeInformation provided by HexCel