Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 9.55 GPa | 1390 ksi | |
Plastcom SLOVAMID 6 GF 25 FRG 5 PA6, 25% glass fibre, flame retardant FeaturesPA 6 for injection moulding, chemically reinforced with 25% glass fibre, with nonhalogen flame retardant. Main features: flammability in accordance with UL 94 V0 at 1.6 mm, glow wire at 960°.. |
|||
Tensile Modulus | 9.55 GPa | 1390 ksi | 1 mm/min; ISO 527-1,-2 |
Gromax BFG30-FU00B3 Nylon 6 30% Glass Filled (Dry) Information provided by Gromax Enterprises Corp. |
|||
Tensile Modulus | 9.55 GPa | 1390 ksi | 1 mm/min; ISO 527-1,-2 |
Gromax BFG30-AH00B3 Nylon 6 30% Glass Filled (Dry) Information provided by Gromax Enterprises Corp. |
|||
Tensile Modulus | 9.55 GPa | 1390 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics LNP VERTON MV008S PP LNP VERTON* MV008S is a compound based on Polypropylene resin containing 40% Long Glass Fiber. Added features of this material include: Chemically Coupled, Heat Stabilized, Structural. |
|||
Tensile Modulus | 9.55 GPa | 1390 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics LNP VERTON MV008S PP (Asia Pacific) LNP VERTON* MV008S is a compound based on Polypropylene resin containing Long Glass. Added features of this material include: Chemically Coupled. |
|||
Tensile Modulus | 9.55 GPa | 1390 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics LNP VERTON MV008S PP (Europe-Africa-Middle East) LNP VERTON* MV008S is a compound based on Polypropylene resin containing Long Glass. Added features of this material include: Chemically Coupled, Heat Stabilized. |
|||
Tensile Modulus | 9.55 GPa | 1390 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics LNP VERTON MV008SU PP LNP VERTON* MV008SU is a compound based on Polypropylene resin containing 40% Long Glass Fiber. Added features of this material include: Chemically Coupled, Heat Stabilized, UV Stabilized, Structur.. |
|||
Tensile Modulus | 9.55 GPa | 1390 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics LNP VERTON MV008SU PP (Asia Pacific) LNP VERTON* MV008SU is a compound based on Polypropylene resin containing Long Glass. Added features of this material include: Chemically Coupled. |
|||
Tensile Modulus | 9.55 GPa | 1390 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics LNP VERTON MV008SU PP (Europe-Africa-Middle East) LNP VERTON* MV008SU is a compound based on Polypropylene resin containing Long Glass. Added features of this material include: Chemically Coupled, Heat Stabilized, UV-Stabilized. |
|||
Tensile Modulus | 9.55 GPa | 1390 ksi | ISO 527 |
BASF Ultramid® A3EG6 BK 00564 PA66 (Dry) Information provided by BASF |
|||
Tensile Modulus | 9.55 GPa | 1390 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics LNP VERTON MV008SXP PP (Europe-Africa-Middle East) LNP* Verton* MV008SXP is a compound based on Polypropylene resin containing Long Glass. Added features include: Chemically Coupled, Heat Stabilized. |