Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

BASF Ultramid® A3EG6 BK 00564 PA66 (Dry)

Category Polymer , Thermoplastic , Nylon , Nylon 66
Manufacturer BASF
Trade Name Ultramid®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF BASF Ultramid® A3EG6 BK 00564 PA66 (Dry).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information provided by BASF
Physical Properties Metric English Comments
Density 1.36 g/cc
0.0491 lb/in³
ISO 1183
Moisture Absorption at Equilibrium 1.7 %
1.7 %
50% RH; ISO 62
5.5 %
5.5 %
Saturation; ISO 62
Mechanical Properties Metric English Comments
Tensile Strength at Break 170 MPa
24700 psi
ISO 527
Elongation at Break 2.5 %
2.5 %
ISO 527
Tensile Modulus 9.55 GPa
1390 ksi
ISO 527
Flexural Modulus 8.55 GPa
1240 ksi
ISO 178
Charpy Impact, Notched 0.700 J/cm²
3.33 ft-lb/in²
ISO 179
Thermal Properties Metric English Comments
Melting Point 260 °C
500 °F
ISO 3146
Deflection Temperature at 0.46 MPa (66 psi) 260 °C
500 °F
ISO 75
Deflection Temperature at 1.8 MPa (264 psi) 250 °C
482 °F
ISO 75
Descriptive Properties Value Comments
Color BK 00564
Commercial Status North America
Users viewing this material also viewed the following: