Mechanical Properties Metric English Comments
Tensile Modulus 6.49 GPa
941 ksi
1 mm/min; ISO 527
SABIC Innovative Plastics LNP Thermocomp FF008L PE
LNP* Thermocomp* FF008L is a compounding based on Polyethylene containing glass fiber. Added characteristics include Low Extractible.This data was supplied by SABIC-IP for the Americas region.
Tensile Modulus 6.49 GPa
941 ksi
1 mm/min; ISO 527
SABIC Innovative Plastics LNP THERMOCOMP LF002 PEEK
LNP* THERMOCOMP* LF002 is a compound based on Polyetheretherketone resin containing 10% Glass Fiber.