Tensile Modulus 67.0 GPa
9720 ksi
EN2597B
Hexcel® HexPly® M56 180°C (350°F) Out-of-Autoclave Curing Matrix, M56/40%/285T2/AS4C-6K
Fiber: AS4C, Weave: 2x2T, 295 g/m2Information provided by HexCel
Tensile Modulus 67.0 GPa
9720 ksi
Material as cured; RT
Hexcel® HexPly® 922-1/35%/G926 180°C Curing Epoxy Matrix
5H satin/370g/m2 carbon fabric: FVC=60%Information provided by HexCel
Tensile Modulus 67.0 GPa

@Temperature 23.0 °C
9720 ksi

@Temperature 73.4 °F
prEN2561 Type B
Hexcel® HexPly® M48 180°C/356°F Curing Epoxy Matrix, M48/42%/G1094/1000
Fiber: T800H 6K, 5H Satin weave, 290 g/m2Information provided by HexCel