Polymer Property : Tensile Modulus = 985 ksi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Modulus 6.79 GPa
985 ksi
1 mm/min; ISO 527
SABIC Innovative Plastics LNP THERMOCOMP IF004 PA6.12
LNP* THERMOCOMP* IF004 is a compound based on Nylon 6/12 resin containing 20% Glass Fiber.
Tensile Modulus 6.79 GPa
985 ksi
ASTM D638
Plenco 51015 PET, Pellet, Injection Molded, Black  (discontinued **)
PLENCO 51015 is an engineering grade glass reinforced recycled polyethylene terephthalate resin designed for increased flexibility and good physical strength. It is UL listed.Information supplied by..