Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 6.80 GPa | 986 ksi | |
Plastcom SLOVAMID 6 GF 5 T 20 FRG 2 PA6, 5% glass fibre, 20% mineral filling FeaturesPA 6 for injection moulding, with halogen free flame retardant based on polyphosphate. Good anisotrophi shinking. Application for the electrical industry: protectors, coil forms, covers, ter.. |
|||
Tensile Modulus | 6.80 GPa | 986 ksi | STN EN ISO 527-2 |
Plastcom SLOVAMID 6 GF 20 Polyamide 6, 20% Glass Fiber FeaturesPA 6 for injection moulding, chemically coupled with 20% glass fiber. Application: impacted mouldings and mouldings with high strength applied in automotive, electrical, engineering and con.. |
|||
Tensile Modulus | 6.80 GPa | 986 ksi | ISO 527 |
Nilit FRIANYL A63 CV-CU 0550 Nylon 6.6 for injection molding, 5% carbon fiber reinforced, 50% copper filled Nylon 6.6 for injection moldingInformation provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Tensile Modulus | 6.80 GPa | 986 ksi | cond.; ISO 527-1, -2; 1 mm/min |
Lanxess Durethan® BKV 35 H3.0 000000 Nylon 6, Glass Fiber Reinforced PA 6, 35% glass fibers, injection molding, heat-aging stabilizedInformation provided by LANXESS. |
|||
Tensile Modulus | 6.80 GPa | 986 ksi | |
Haveg 61NA Furfuryl Alcohol-Formaldehyde Resin A proprietary thermoset plastic consisting of a furfuryl alcohol-formaldehyde resin and non-asbestos silicate fillers. |
|||
Tensile Modulus | 6.80 GPa | 986 ksi | ISO 527 |
Solvay TECHNYL® A 52 G1 MX 20 PA66, Eh 0 Description: TECHNYL A 52 G1 MX20 is a Polyamide 6.6 glow wire resistant, reinforced with mineral fillerColors: it is marketed in black color.Available in: Latin AmericaMain Properties: ?Glow wire r.. |
|||
Tensile Modulus | 6.80 GPa | 986 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics ULTEM 2200 PEI (Europe-Africa-Middle East) 20% Glass fiber filled, standard flow Polyetherimide (Tg 217C). Resin is RoHS compliant. UL94 V0 and 5VA listing. |
|||
Tensile Modulus | 6.80 GPa | 986 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics ULTEM 2200F PEI (Europe-Africa-Middle East) 20% Glass fiber filled, standard flow Polyetherimide (Tg 217C). Resin is RoHS compliant. US FDA and European Food Contact approved. Effective June, 2007 this grade will no longer be supported with b.. |
|||
Tensile Modulus | 6.80 GPa | 986 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics Ultem 2200N PEI (Asia Pacific) 20% Glass fiber filled Polyetherimide (Tg 217C). ECO Conforming.This data was supplied by SABIC-IP for the Asia Pacific region. |
|||
Tensile Modulus | 6.80 GPa | 986 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics Ultem 2200N PEI (Europe-Africa-Middle East) 20% Glass fiber filled Polyetherimide (Tg 217C). ECO Conforming.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |
|||
Tensile Modulus | 6.80 GPa | 986 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics ULTEM 2210 PEI (Europe-Africa-Middle East) 20% Glass fiber filled, enhanced flow Polyetherimide (Tg 217C). Resin is RoHS compliant. UL94 V0 and 5VA listing. |
|||
Tensile Modulus | 6.80 GPa | 986 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics ULTEM 2210F PEI (Europe-Africa-Middle East) 20% Glass fiber filled, enhanced flow Polyetherimide (Tg 217C). Resin is RoHS compliant. US FDA and European Food Contact approved. Effective June, 2007 this grade will no longer be supported with b.. |
|||
Tensile Modulus | 6.80 GPa | 986 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics ULTEM 2210K PEI (Asia Pacific) 20% Glass fiber filled, enhanced flow Polyetherimide (Tg 217C). ECO Conforming. |
|||
Tensile Modulus | 6.80 GPa | 986 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics Ultem 2210K PEI (Europe-Africa-Middle East) 20% Glass fiber filled, enhanced flow Polyetherimide (Tg 217C). ECO Conforming.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |
|||
Tensile Modulus | 6.80 GPa | 986 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics ULTEM 2210R PEI (Europe-Africa-Middle East) 20% Glass fiber filled, enhanced flow Polyetherimide (Tg 217C) with internal mold release. Resin is RoHS compliant. UL94 V0 and 5VA listing. |
|||
Tensile Modulus | 6.80 GPa | 986 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics Ultem PW2200 PEI (Europe-Africa-Middle East) 20% Glass fiber filled, standard flow Polyetherimide (Tg 217°C). Product designed and certified for use in Potable Water
applications. KTW, WRAS, ACS certified. NSF61 and W270 pending. US FDA and.. |
|||
Tensile Modulus | 6.80 GPa | 986 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP STAT-KON DE002ER PC LNP STAT-KON* DE002ER is a compound based on Polycarbonate resin containing 10% Carbon Fiber. Added features of this material include: Easy Molding. Mold Release, Electrically Conductive. |
|||
Tensile Modulus | 6.80 GPa | 986 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP STAT-KON DE002ER PC (Asia Pacific) LNP STAT-KON* DE002ER is a compound based on Polycarbonate resin containing Carbon Fiber. Added features of this material include: Easy Molding. |
|||
Tensile Modulus | 6.80 GPa | 986 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP THERMOCOMP CX05470 PS LNP* THERMOCOMP* CX05470 is a compound based on Polystyrene resin containing 20% Glass Fiber. |
|||
Tensile Modulus | 6.80 GPa | 986 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP THERMOCOMP EF004 PEI LNP* Thermocomp* EF004 is a compound based on Polyetherimide resin containing 20% Glass Fiber. |
|||
Tensile Modulus | 6.80 GPa | 986 ksi | 1 mm/min; ISO 527-1 |
Sax Polymers SAXAMID 136F6Q32 Nylon 6, 30% Glass Fiber SAXAMID 136F6Q32 is a high-impact-modified polyamide 6 injection-molding-grade reinforced with 30% glass fibers . Beside the high impact strength at low temperatures this grade shows very good proce.. |
|||
Tensile Modulus | 6.80 GPa | 986 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics NORYL GTX GTX8120P PPE+PA (Europe-Africa-Middle East) GTX8120P is a glass filled extrudable Noryl GTX with low thermal conductivity, suitable for thermal breaks |
|||
Tensile Modulus | 6.80 GPa | 986 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics NORYL NH7114 PPE+HIPS Noryl* NH7114 resin is a 20% glass reinforced, modified PPE-PS blend. The material uses non-halogenated flame retardants to achieve UL94 flame ratings while offering an exceptional balance of streng.. |
|||
Tensile Modulus | 6.80 GPa | 986 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics NORYL NH7114 PPE+HIPS (Asia Pacific) Noryl* NH7114 resin is a 20% glass reinforced, modified PPE-PS blend. The material uses non-halogenated flame retardants to achieve UL94 flame ratings while offering an exceptional balance of streng.. |
|||
Tensile Modulus | 6.80 GPa | 986 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics NORYL NH7114 PPE+HIPS (Europe-Africa-Middle East) Noryl* NH7114 resin is a 20% glass reinforced, modified PPE-PS blend. The material uses non-halogenated flame retardants to achieve UL94 flame ratings while offering an exceptional balance of streng.. |
|||
Tensile Modulus | 6.80 GPa | 986 ksi | dry; ISO 527 |
Ter Hell Plastic Terez® PA 6 7500 TF 20 GF 20 Polyamide 6, 20% PTFE chemically bonded 20% glass fiber reinforced Description: Medium viscosity PA 6, 20% PTFE chemically bonded and 20% glass fiber reinforced, good flowability, good impact resistance and bright natural color.Application: For molding parts with.. |
|||
Tensile Modulus | 6.80 GPa | 986 ksi | ISO 527 |
CP-Polymer-Technik Wellamid® 6000 GV 30 HWCP 30% Glass Fiber Nylon 6, Heat Stabilized, Conditioned Information provided by CP-Polymer-Technik GmbH & Co. KG |
|||
Tensile Modulus | 6.80 GPa | 986 ksi | ISO 527-1/-2 |
DuPont Performance Polymers Rynite® FR515 NC010 Polyethylene Terephthalate (PET)
(Unverified Data**) 15% Glass Reinforced Flame Retardant Polyethylene Terephthalate Rynite FR515 NC010 is a flame retardant 15% glass reinforced modified polyethylene terephthalate. Recognized by UL as UL94V-0 at 0.8mm.. |