Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Fracture Toughness | 2.63 MPa-m½ | 2.39 ksi-in½ | |
Poco Graphite SUPERSiC® Si Silicon Carbide The SUPERSiC Material System allows customization of basic silicon carbide. Select from groups of infiltration materials, cleaning options, coating materials and thicknesses to optimize material for.. |
|||
Fracture Toughness | 2.63 MPa-m½ | 2.39 ksi-in½ | |
Poco Graphite SUPERSiC® Si-3C Silicon Carbide SUPERSiC that has been infiltrated with silicon and then coated with a 75 µm CVD SiC coating, sealing off the porosity.Uses: Ideal for high-temperature vacuum CVD systemsInformation provided by Poc.. |
|||
Fracture Toughness | 2.63 MPa-m½ | 2.39 ksi-in½ | |
Poco Graphite SUPERSiC® Si-8C Silicon Carbide SUPERSiC that has been infiltrated with silicon and then coated with a 200 µm CVD SiC coatingUses: Ideal for optical and lithography componentsInformation provided by Poco Graphite |