Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Shear Modulus | 0.0110 GPa | 1.60 ksi | Plate Shear, W Direction, typ |
Hexcel® HexWeb® HRH-10 - 3/16 - 1.5 Aramid Fiber/Phenolic Resin Honeycomb Designation: Material-Cell Size-Density.Hexweb HRH-10 is manufactured from NOMEX aramid fiber sheets. A thermosetting adhesive is used to bond these sheets at the nodes, and after expanding to the h.. |
|||
Shear Modulus | 0.0110 GPa | 1.60 ksi | average; ASTM C393 |
3A Composites Core Materials AIREX® R63.50 Damage Tolerant Foam AIREX® R63 is a closed-cell, linear, thermoplastic polymer foam with high damage tolerance. This one of a kind formula combines very high elongation and excellent bond strength. AIREX® R63 is cold.. |