Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Shear Modulus | 0.0165 GPa | 2.40 ksi | Plate Shear, W Direction, typ |
Hexcel® HexWeb® HRH-10 - 3/8 - 2.0 Aramid Fiber/Phenolic Resin Honeycomb Designation: Material-Cell Size-Density.Hexweb HRH-10 is manufactured from NOMEX aramid fiber sheets. A thermosetting adhesive is used to bond these sheets at the nodes, and after expanding to the h.. |