Mechanical Properties Metric English Comments
Shear Modulus 0.0248 GPa
3.60 ksi
Plate Shear, W Direction, typ
Hexcel® HexWeb® HRH-10/F50 - 3.5 Nonmetallic Flex-Core Honeycomb
Designation: Material/Cell Size (cells per lineal foot in W direction)-DensityHexcel manufactures two types of nonmetallic reinforced plastic HexWeb Flex-Core: HexWeb HRP - Fiberglasses cloth reinfo..