Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Shear Modulus | 0.0248 GPa | 3.60 ksi | Plate Shear, W Direction, typ |
Hexcel® HexWeb® HRH-10/F50 - 3.5 Nonmetallic Flex-Core Honeycomb Designation: Material/Cell Size (cells per lineal foot in W direction)-DensityHexcel manufactures two types of nonmetallic reinforced plastic HexWeb Flex-Core: HexWeb HRP - Fiberglasses cloth reinfo.. |