Mechanical Properties Metric English Comments
Shear Modulus 0.150 GPa
21.8 ksi
BASF Elastollan® 1164D Polyether Type Polyurethane Elastomer
Recommended for injection molding. Elastollan ® 1100 series products are FDA Sec. 177.2600 compliant. Elastollan 1100 series of products are polyether-based thermoplastic polyurethanes. They exhi..