Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Shear Modulus | 0.852 - 6.74 GPa | 124 - 978 ksi | Average value: 3.53 GPa Grade Count:15 |
Overview of materials for Polyphthalamide (PPA) This property data is a summary of similar materials in the MatWeb database for the category "Polyphthalamide". Each property range of values reported is minimum and maximum values of appropriate Ma.. |
|||
Shear Modulus | 0.852 - 0.889 GPa | 124 - 129 ksi | Calculated |
Solvay Specialty Polymers Amodel® ET-1001 L Polyphthalamide (PPA) Resin, Dry as Molded
(discontinued **) AMODEL ET-1001 L resin is an impact modified polyphthalamide (PPA) with exceptional impact strength and practical toughness. AMODEL PPA resins offer high fatigue strength, and good chemical resistan.. |