Mechanical Properties Metric English Comments
Shear Modulus 0.0250 - 0.950 GPa

@Temperature 50.0 - 200 °C
3.63 - 138 ksi

@Temperature 122 - 392 °F
Average value: 0.669 GPa Grade Count:1
Overview of materials for Polysulfone, 20% Glass Fiber Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "Polysulfone, 20% Glass Fiber Reinforced". Specific grades with glass content between 15% and 24% are inc..
Shear Modulus 0.0250 - 0.950 GPa

@Temperature 50.0 - 200 °C
3.63 - 138 ksi

@Temperature 122 - 392 °F
Average value: 0.669 GPa Grade Count:1
Overview of materials for Polysulfone, 30% Glass Fiber Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "Polysulfone, 30% Glass Fiber Reinforced". Specific grades with glass content between 25% and 34% are inc..