Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Shear Modulus | 0.0250 - 0.950 GPa @Temperature 50.0 - 200 °C |
3.63 - 138 ksi @Temperature 122 - 392 °F |
Average value: 0.669 GPa Grade Count:1 |
Overview of materials for Polysulfone, 20% Glass Fiber Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Polysulfone, 20% Glass Fiber Reinforced". Specific grades with glass content between 15% and 24% are inc.. |
|||
Shear Modulus | 0.0250 - 0.950 GPa @Temperature 50.0 - 200 °C |
3.63 - 138 ksi @Temperature 122 - 392 °F |
Average value: 0.669 GPa Grade Count:1 |
Overview of materials for Polysulfone, 30% Glass Fiber Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Polysulfone, 30% Glass Fiber Reinforced". Specific grades with glass content between 25% and 34% are inc.. |